Sm3+-doped Li2Cd2(PO4)2 (LCP) nanopowders were prepared using solid state reaction (SSR) method. Several analytical methods were used to examine the prepared samples structural, morphological, vibrational and luminous characteristics. The XRD analysis reveals that the samples were in the orthorhombic with Pnma space group in the nanoscale. The average crystallite size for the samples were determined using Debye Scherrer’s and W-H plot methods. Surface morphology revealed an irregular stone-like clustered architecture. FT-IR and Raman spectroscopy were employed to investigate the vibrational characteristics of the samples. DRS analysis estimated optical bandgap values of 5.43 eV for the undoped sample and 5.01, 5.05, and 5.19 eV for the 0.01%, 0.05%, and 0.09% Sm3+-doped LCP samples, respectively. The photoluminescence spectrum exhibited a prominent emission at 649 nm upon excitation at 401 nm. Concentration quenching behaviour, average lifetime, quantum yield, correlated colour temperature (CCT), colour purity (CP) and colour rendering index (CRI) were systematically evaluated. The optical characteristics indicate that the developed Sm3+-doped LCP phosphors possess strong potential for application in reddish-orange light-emitting devices.
The polyol synthesis method was employed to prepare LaInO3 perovskite phosphors doped with Bi3+ (x = 1, 3, 5 at.%) and co-doped with Dy3+ (y = 1-5 at.%). The X-ray diffraction (XRD) confirmed the formation of a pure orthorhombic LaInO3 phase in annealed samples. Morphological analysis revealed spherical agglomerates with some irregularities, ranging in size from 60 to 90 nm. The reduction of energy band gap on doping ions into lattice using DFT studies. The energy-dispersive spectroscopy (EDS) confirmed the successful incorporation of Bi3+ and Dy3+ ions into the LaInO3 lattice. The photoluminescence (PL) studies demonstrated that Bi3+-doped LaInO3 exhibited a broad blue emission peak at 432 nm due to the 3P1→1S0 transition of Bi3+ ions. On the other hand, LaInO3 doped with Dy3+ exhibited distinctive emissions at 482 nm (blue) and 584 nm (yellow), which correspond to the 4F9/2→6H15/2 and 4F9/2→6H13/2 transitions of Dy3+ ions, respectively. The optimized sample composition is found to be LaInO3: 3 at.% Bi3+, 3 at.% Dy3+ demonstrated enhanced emission intensities due to energy transfer from Bi3+ to Dy3+ ions making it a promising candidate for advanced LED applications.