Representative Publications

View All Publications
1 January 2021 in Journal of Magnesium and Alloys
Verified
Journal Article
Open access
AGA. Gungor
A. Gungor
AIA. Incesu
A. Incesu

28 November 2020 in Journal of Materials Science: Materials in Medicine
Verified
Journal Article
Closed access
PDF file
AIAlper Incesu
Alper Incesu
AGAli Gungor
Ali Gungor

1 October 2018 in Journal of Alloys and Compounds
Verified
Journal Article
Closed access
HEHamid Ali Elamami
Hamid Ali Elamami
AIAlper Incesu
Alper Incesu
KKKonstantinos Korgiopoulos
Konstantinos Korgiopoulos
MPMihriban Pekguleryuz
Mihriban Pekguleryuz
AGAli Gungor
Ali Gungor

3 April 2015 in Advances in Materials and Processing Technologies
Verified
Journal Article
Closed access
AIAlper Incesu
Alper Incesu
AGA. Gungor
A. Gungor
In this study, influence of different heat treatment conditions on microstructure, microhardness, yield strength, ultimate tensile strength, elongation and phase distribution of AZ63 magnesium alloy were discussed. All specimens were taken from as cast commercial AZ63 magnesium alloy. Solution heat treatment was applied at 400 °C for 16 h. After air cooling the specimens to room temperature, the specimens were aged at two different temperatures; 160, 190 °C and five different durations; 1, 3, 6, 9 and 12 h. The effects of heat treatment conditions on the mechanical and microstructural properties of AZ63 magnesium alloy were determined by tensile and microhardness tests, SEM, EDX and XRD analyses, respectively. It was observed that, after the solution treatment, a weak intermetallic phase of Mg17Al12 was dissolved almost totally in the matrix. During ageing, this phase precipitated in the grains and also on the grain boundaries homogeneously depending on the ageing temperatures and times.

7 November 2024 in Journal of Metals, Materials and Minerals
Verified
Journal Article
Open access
PDF file
HEHalil Eren
Halil Eren
AGAli Güngör
Ali Güngör
EKErkan Koç
Erkan Koç
HÇHarun Çuğ
Harun Çuğ
In this study, it was aimed to develop a biodegradable metallic plate that is an alternative to bioinert metal plates. The main advantage of using biodegradable materials for implants is that they can be gradually replaced with the patient's own tissue, which reduces the need for additional surgeries to remove the implant after it has served its purpose. Magnesium and its alloys can provide biocompatibility as orthopedic implant materials. Mg-Zn-Ca and Mg-Zn-Ca-Sn alloys were prepared using the gravity die casting method. Zn (1.0 wt% and 2.0 wt%) and Sn (0.0 wt%, 0.5 wt% and 1.0 wt%) ratios were used as variables, and the Ca ratio (0.3 wt%) was kept constant in all alloys. After homogenization heat treatment, alloys were hot rolled. Hot rolling resulted in grain refinement, much higher yield and tensile strength, and hardness at the expense of the lower strain. However, hot rolling had a detrimental impact on the corrosion resistance of the alloys. Among the alloys, ZX20-h alloy showed the highest yield and tensile strength before and after corrosion tests. The lowest corrosion rate was measured in ZXT200 alloy as 5.1 mm∙year‒1 after 10 day of immersion. Although ZX20-h alloy has a higher corrosion rate (13.56 mm∙year‒1) than ZXT200 alloy, it can be improved further to be used as biodegradable bone support plate material.

1 September 2022 in Gazi University Journal of Science
Verified
Journal Article
Closed access
PDF file
AIAlper İnCesu
Alper İnCesu
AGAli Güngör
Ali Güngör
In this study, hot rolling is properly performed on pure magnesium and two of Zn, Ca and Mn containing magnesium alloys. Biodegradability and mechanical properties are investigated comparatively in their rolled state. While the average grain sizes of the two alloys were close to each other, it was observed that the Mg-1.01Zn-1.63Ca-0.30Mn alloy had higher hardness (61.5 ± 0.2 HV) at hot rolled state. The lowest corrosion rate in electrochemical corrosion test on Mg-1.07Zn-0.21Ca-0.31Mn alloy is observed to be 1.772 mm/yr. As for the immersion corrosion test on the same alloy, the lowest corrosion rate is detected to be 0.054 mm/yr. Moreover, Mg-1.07Zn-0.21Ca-0.31Mn alloy has the highest tensile strength. Based on the results, it is ascertained that hot-rolled Mg-1.07Zn-0.21Ca-0.31Mn alloy possesses a better biodegradability and mechanical properties compared to hot rolled commercially unalloyed Mg and 1.01Zn-1.63Ca-0.30Mn alloy.