15 March 2019 in Journal of the Electrochemical Society
This paper studied the gases release of a graphite//NMC111(LiNi1/3Mn1/3Co1/3O2) cell during cycle in the voltage ranges of 2.6-4.2V and 2.6-4.8V and the temperatures of at 25°C and 60°C. It was proved that the CO2, CO, and H2 gases are released as a result of electrolyte decomposition. And it shows that the CO and H2 gases evolution is a direct consequence of the electrochemical reaction of electrolyte decomposition, while the CO2 generation is a consequence of the additional chemical reaction of interaction between the O2 released from the cathode atomic lattice oxygen and CO released from the same place on the cathode (appearing because of the electrolyte decomposition). That is why at the same electrochemical reaction of electrolyte decomposition, the ratio CO2/CO varies in the wide range from 0.82 to 2.42 depending on cycling conditions (temperature and cutoff voltage). It was proved that a potential-independent H2 evolution is a consequence of its adsorption in pores of powdered graphite on anode. There was proposed the mechanism of the electrolyte decomposition and the gases evolution in lithium-ion cells at their cycling, which corresponds quantitatively to all obtained experimental results.
28 July 2015 in Journal of the Electrochemical Society
In this investigation, there was deduced from experiments that an exothermic reaction in the thermal runaway process in alkaline batteries is the electrochemical reaction of atomic hydrogen recombination Hads Cd + Hads Ni → H2↑(H2O + Hads + e- → H2↑ + OH- on a cathode and Hads + OH- → H2O + e- on an anode). A rate-limiting step for this reaction on both a cathode and an anode is found to be a step of metal-hydrides disintegration. This electrochemical reaction proceeds at voltage 0.5–0.6 V on battery terminals according to experimental data on the thermal runaway. The possible thermal runaway mechanism has been proposed corresponding to all the experimental results obtained.
1 March 2008 in Journal of Power Sources
23 January 2015 in Journal of the Electrochemical Society
It was shown on the basis of charge current, terminal voltage, and change in battery temperature that during thermal runaway, the observed changes cannot be explained by the self-acceleration of known reactions (due to overheating), battery charging and electrolyte decomposition. The observed changes can only be explained if we assume, that the thermal runaway is associated with a powerful electrochemical reaction going within the battery with a terminal voltage approximately 0.55 V. It is shown that the recombination reaction of atomic hydrogen accumulated in the electrodes is exothermic thermal runaway reaction in alkaline batteries. New mechanism of thermal runaway in Ni-Cd batteries, which explains all the experimental data known currently is proposed.
1 November 2014 in International Journal of Hydrogen Energy
1 September 2016 in International Journal of Hydrogen Energy