The particle shape and size of the starting powders represent the most important physical properties, on which the quality of the compacts and final sintered products depends. Two types of powder were analyzed in the paper - electrolytic copper powder with a dendritic particle shape and water-atomized copper powder with an irregular particle shape. The starting powders were sieved through a sieve system with openings of 45 μm, 80 μm, and 120 μm. The characterization of the obtained fractions of both powders was performed by determining the shape and dimensions of the particles using SEM microscopy in combination with ImageJ software, and the apparent density and flow rate were determined using the Hall flowmeter funnel. Pressing of each powder fraction was done using a pressure of 600 MPa. The compacts were further sintered at 1000°C for 2 hours to obtain the final sintered parts. After sintering, their density, hardness, and electrical conductivity were determined and their microstructure was analyzed. The results indicate a great influence of the characteristics of the starting powders on the properties of the final parts obtained by the powder metallurgy route. The particle shape of the powders had a more pronounced influence compared to the particle size.
Development of various types the so-called "environmentally friendly" solders has been extensively investigated worldwide as an alternative to the lead-based solders. This study investigated the impact of graphene nanoparticles on microstructure and thermal properties of the lead-free solders. The nanocomposite solders were produced using the powder metallurgy method. The graphene nanoparticles were used as the reinforcement in the form of graphene nanosheets (GNS). The microstructural analysis showed that the GNS particles were homogeneously distributed along the grain boundaries, resulting in a refined b-Sn structure. At room temperature, density was measured using the Archimedes method, while the thermal diffusivity was determined using the flash method. The thermal conductivity of the Sn-0.7Cu nanocomposite solders was calculated using a fundamental equation. Increasing the GNS content up to 0.08 wt% in the Sn-0.7Cu solder matrix led to a slight decrease in density of the nanocomposite solders compared to the base solder, while the highest thermal conductivity was achieved with a 0.05 wt% GNS addition, reaching 44.74 Wm⁻¹ K⁻¹.
The aim of this work is to analyze the process of obtaining and thermal treatment on the grain size of copper microalloyed with iron and phosphorus (0,003 wt%Fe i 0,014 wt%P). Microalloyed copper was obtained in two ways: by melting cathode copper and prealloys CuFe0,1 and CuP6,42 in an induction furnace followed by the casting of the same raw materials and the up-casting process, followed by extrusion. The samples obtained in this way were subjected to thermomechanical treatment, which involved cold plastic deformation by rolling with 70% reduction, followed by annealing at 470°C for 80 minutes. Based on the microphotographs and the ImageJ software, the average grain size and grain size distribution were determined for each tested sample. The results showed that the average grain size of the extruded sample was smaller, and the microstructure was more uniform and had a higher degree of recrystallization, which can be attributed to severe plastic deformation (extrusion).
This study investigates the influence of heat input during oxy-fuel cutting on the microstructure and hardness of high-carbon steel. The material analyzed was a steel bar designed for use in mining mills, processed through this thermal cutting technique. After cutting, a detailed metallographic analysis of the heat-affected zone (HAZ) was carried out using optical microscopy, while Vickers hardness (HV20) was measured at various distances from the cut edge. The results showed that, due to the high temperatures generated during cutting, significant structural changes occurred within the HAZ. At the surface edge, hardness measurements revealed a slight increase, indicating localized hardening associated with rapid cooling and the resulting microstructural changes. The obtained results were compared with relevant literature data, providing a deeper understanding of the thermal effects on the microstructure in this type of steel.
The effect of graphene nanosheets (GNS) on the wettability and microstructure of Sn-0.7Cu-xGNS (x = 0, 0.02, 0.04, 0.06, 0.08, and 0.1 wt.%) nanocomposite solders was investigated. The composites were produced using the powder metallurgy (PM) technique. The microstructures of the solder joints between the solders and copper substrates were examined using a scanning electron microscope (SEM), and the presence of intermetallic compounds (IMCs) was confirmed by energy-dispersive spectroscopy (EDS). The thickness of the intermetallic layer formed at the solder/Cu interface was reduced by 64.6% with the addition of up to 0.1 wt.% GNS, compared to the Sn-0.7Cu base solder. The wettability of the samples was evaluated by measuring the spreading area of the solders on the copper substrates. The results showed that the addition of up to 0.1 wt.% GNS significantly improved wettability, as evidenced by a 95.2% increase in spreading area compared to the unreinforced solder.
This work includes experimental studies of the influence of thermomechanical processing regime on the mechanical properties of CuFe1 alloy, in the form of a wire Ø1,0 mm. The CuFe1 alloy was melted and homogenized in a medium-frequency induction crucible furnace, and casting was performed by the crystallization method above the melt using a casting machine. The resulting cast wire Ø8,0 mm was drawn on a multi-stage drawing machine according to a drawing plan identical to the Cu wire. Interphase annealing was performed at a temperature of 650 °C in a bell furnace with a protective nitrogen atmosphere for 1 hour. Final annealing of the samples was carried out at temperatures of 320, 400, 450, 500, 550, 650 and 800 °C for 1h and 0,5h. By combining temperatures and annealing times, the aim was to achieve a primarily appropriate elongation value (A ≥ 25 %) dictated by the exploitation conditions in which this wire is used. The results showed that the optimal conditions for the required mechanical characteristics of the material, primarily elongation, were achieved at an annealing temperature of 650 °C for a time duration of 0,5h.