20 August 2024 in International Journal of Building Pathology and Adaptation
Purpose: This paper aims to investigate the bond strength of metakaolin-based geopolymer mortar with cement mortar.Design/methodology/approach: The mortar-mortar bond strength is assessed by slant shear and split tensile tests; pure shear strength is evaluated by Mohr’s criterion for result validation. Metakaolin-based geopolymer mortar is cast over the cured cement mortar specimen with two levels of surface roughness: smooth or grooved interface. The influence of the alkaline solution to metakaolin ratio on geopolymer bond strength is studied. Compressive strength, ultrasonic pulse velocity, permeability and flow table tests are also performed.Findings: The paper’s findings are highlighted as follows: (1) strong mortar-mortar bond properties achieved for geopolymer mortar in all tests and conditions and validated by Mohr’s criterion and pure shear, (2) a lower alkaline solution to metakaolin ratio achieves higher bond strength to Portland cement mortar and (3) geopolymer mortar has higher compressive strength and ultrasonic pulse velocity than cement mortar at all curing ages; additionally, it is more flowable and less permeable.Practical implications: The full replacement of Portland cement with metakaolin, a more sustainable cementitious material, will contribute to the decarbonization of the construction industry.Originality/value: Limited research has been carried out on the bond strength of metakaolin-based geopolymer mortar to Portland cement mortar. Also, computing the pure shear using Mohr’s circle criterion of metakaolin-based geopolymer to validate the results can be considered original.
3 November 2025 in Engineering Reports
MDMohamad Ezzedine El Dandachy
Mohamad Ezzedine El Dandachy
This research examines the interfacial bond strength of metakaolin‐based geopolymer mortar across two key connections: flexural mortar–mortar and steel–mortar. It investigates the effect of interfacial roughness and curing age on the bond behavior of metakaolin‐based geopolymer mortar (GPM) and cement‐based mortar (CM). In this research, the mortar‐to‐mortar bond strength was assessed using the flexural three‐point bending test on smooth and grooved interfaces after 28 + 7 and 28 + 28 days of curing, complementing previous slant shear and split tensile test results. For the steel–mortar investigation, push‐in tests were conducted on 10 mm diameter ribbed and 8 mm diameter smooth steel reinforcing bars, with 7 and 28 days of curing for each. Additional tests included compressive strength, ultrasonic pulse velocity, and drying shrinkage, alongside previous bond strength research using the slant shear and split tensile tests. Results demonstrate that geopolymer mortar achieves superior bond strength compared to cement mortar, with bond strengths more than double that of cement mortar. Geopolymer mortar also attained faster bond strength on grooved surfaces. Similarly, the steel–mortar bond strength of metakaolin‐based geopolymer mortar was approximately four times greater than that of cement mortar with ribbed rebars, although results were closer with smooth rebars. These findings highlight the potential of metakaolin‐based geopolymer mortar to enhance bond performance while reducing environmental impact, presenting a promising avenue for sustainable construction practices.