The widespread application of green hydrogen production technologies requires cost reduction of crucial elements. To achieve this, a viable pathway to reduce the iridium loading in proton exchange membrane water electrolysis (PEMWE) is explored. Herein, a scalable synthesis method based on a photodeposition process for a TiO2@IrOx core–shell catalyst with a reduced iridium content as low as 40 wt.% is presented. Using this synthesis method, titania support particles homogeneously coated with a thin iridium oxide shell of only 2.1 ± 0.4 nm are obtained. The catalyst exhibits not only high ex situ activity, but also decent stability compared to commercially available catalysts. Furthermore, the unique core–shell structure provides a threefold increased electrical powder conductivity compared to structures without the shell. In addition, the low iridium content facilitates the fabrication of sufficiently thick catalyst layers at decreased iridium loadings mitigating the impact of crack formation in the catalyst layer during PEMWE operation. It is demonstrated that the novel TiO2@IrOx core–shell catalyst clearly outperforms the commercial reference in single‐cell tests with an iridium loading below 0.3 mgIr cm−2 exhibiting a superior iridium‐specific power density of 17.9 kW gIr−1 compared to 10.4 kW gIr−1 for the commercial reference.
The widespread use of proton exchange membrane water electrolyzers (PEMWE) is hindered by their high cost, of which a colossal factor is caused by the bipolar plates (BPP). In this paper, we investigate the stability of two BPP materials on‐line with an optimized scanning flow cell setup coupled to an inductively coupled plasma mass spectrometer (SFC‐ICP‐MS), as well as scanning electron microscopy (SEM). The stability of currently used titanium and a cheaper alternative, stainless steel (SS) 316L, were characterized in deionized (DI) water and 0.5 mM H2SO4 to mimic the conditions at the BPP under operation. We show that the dissolution of Ti is negligible, whereas SS 316L degrades notably. Here, besides pH, the applied potentials play a crucial role. Nonetheless, even for the highest measured dissolution rate of SS 316L, the contamination in a full cell is estimated to remain below 1 ppm. This work illustrates the capabilities of on‐line high‐throughput stability tests for BPP materials and could therefore contribute towards optimization of cost‐effective PEMWE.
1 April 2024 in Journal of the Electrochemical Society
The interface design between anode catalyst layer (ACL) and porous transport layer (PTL) significantly influences the performance of proton exchange membrane water electrolyzers. Lately, the influence of the ACL/PTL interface on performance is more intensively investigated, including modeling approaches. Contrary to other models that apply through-plane resolved modeling, in-plane models better characterize the ACL/PTL interface. These models separate the interface into three domains: in an open pore area (P), under a contacted solid of the PTL (S), and the interfacial point between the pore and solid (S│P). In our work, we focused on the behavior of the model in the kinetic region, in which no two-phase behavior is to be expected. Consequently, we apply a one-phase model as the main model and a simple two-phase model for comparison. We find that for most reference samples, the one-phase model well describes polarization behavior. However, for samples with larger interfacial contact area, a two-phase model might explain the found effect better even for very low current densities. Finally, we show that the one-phase model and the simple two-phase model can be used to study the general behavior of different solid to pore ratios to guide electrode development in the future.
Stainless steel is a promising material for bipolar plates (BPP) in proton exchange membrane water electrolysis (PEMWE) that could drastically reduce stack costs. However, dissolution of Fe from stainless steel BPP might trigger membrane degradation, which releases fluoride. Fluoride in turn could accelerate stainless steel corrosion. Therefore, the influence of fluoride contamination (namely 0, 1, 5, and 20 ppm in 0.5 mM H 2 SO 4 ) on the dissolution stability of stainless steel (316L) is investigated utilizing a scanning flow cell coupled on‐line to an inductively coupled plasma mass spectrometer (SFC‐ICP‐MS). Fluoride enhances the dissolution exponentially, resulting in enhanced dissolution efficiencies with increased fluoride concentration reaching ≈50% at 20 ppm. Complementary micro and nanostructure analysis (laser profilometry, scanning electron microscopy, and scanning transmission electron microscopy with energy‐dispersive X‐ray spectroscopy) reveals pitting corrosion, whose severity and occurrence appear highly increased with higher fluoride concentration. The results suggest that fluoride impurities in combination with exposed stainless steel, e.g., due to coating imperfections, should be avoided in PEMWE application, as accumulation of impurities of both might lead to a self‐accelerating degradation process.
The widespread application of green hydrogen production technologies requires cost reduction of crucial elements. To achieve this, a viable pathway to reduce the iridium loading in proton exchange membrane water electrolysis (PEMWE) is explored. Herein, we present a scalable synthesis method based on a photodeposition process for a TiO2@IrOx core-shell catalyst with a reduced iridium content as low as 40 wt%. Using this synthesis route, we obtain titania support particles homogeneously coated with a thin iridium oxide shell of only 2.1 ± 0.4 nm. The catalyst exhibits not only high ex situ activity, but also decent stability compared to commercially available catalysts. Furthermore, the unique core-shell structure provides a threefold increased electrical powder conductivity compared to structures without the shell. In addition, the low iridium content facilitates the fabrication of sufficiently thick catalyst layers at decreased iridium loadings mitigating the impact of crack formation in the catalyst layer during PEMWE operation. We demonstrate that the novel TiO2@IrOx core-shell catalyst clearly outperforms the commercial reference in single-cell tests with an iridium loading below 0.3 mgIr cm 2 exhibiting a superior iridium-specific power density of 17.9 kW gIr-1 compared to 10.4 kW gIr-1 for the commercial reference.