The effects of the austenitizing temperature and the cooling rate upon the kinetic of athermal martensitic transformation in a microalloyed steel were evaluated. Considering the studied steel, the knowledge about these effects on the martensitic transformation has a great relevance for naval manufacturers and steel researchers. In this study, computational simulation was performed aiming to evaluate the phase's stability. Specimens were submitted to quenching simulations in a dilatometer, considering four different austenitizing temperatures and four cooling rates. The results shown that the austenite chemical composition was not significantly affected by the austenitizing temperatures. Both the austenitic grain size and the cooling rate affected the martensitic transformation kinetics. The larger the austenitic grain size, the higher the Ms. The austenitic grain growth promoted a decrease in the required chemical energy to compensate the free energy increase associated with the lattice strain and the creation of new interfaces, leading to a lower austenite undercooling. An extrinsic effect of the cooling rate on the Ms was observed. For lower cooling rates, the carbide precipitation modified que austenite chemical composition, changing its stability and increasing Ms. A predictability equation, correlating the M S with the austenite grain size and the steel cooling rate, was proposed.
The transition from upper-to-lower bainite in carbon steels is a complex process yet not fully explored. This study examines such transition in a 0.7C, 0.74Mn, 0.61Si, 0.2Cr (wt%) low-alloy steel using a comprehensive approach that integrates dilatometry, scanning electron microscopy (SEM), ex-situ HEXRD, and microhardness testing. Microhardness and dislocation density were found strongly coupled, both increasing with decreasing austempering temperature and presenting changing trends at approximately 350°C and 300°C. Likewise, an Arrhenius plot derived from the curves of transformed fraction as a function of austempering temperature presented the same behaviour. These turning points are considered, respectively, the onset and the end of the transitional interval between upper and lower bainite. Furthermore, SEM analyses confirmed a progressive change in morphology, from coarse upper bainite at high temperatures (400°C), to a mixture of upper and lower bainite in the transitional range, and finally to exclusively fine lower bainite at low temperatures (275°C). The results support that the upper-to-lower bainite transition is not a discrete step but a continuum and offer insights into the interplay between bainite morphology, overall transformation kinetics, and microhardness, which are critical for optimizing heat treatments routes.