Simon Hammersley

Simon Hammersley

Auto-generated profile, based on publicly available information

Simon Hammersley

University of Manchester 1 School of Physics and Astronomy, Photon Science Institute Manchester M13 9PL, United Kingdom

Research Focus & Metrics

Academic Career Length

17Years (2010-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
15 April 2012 in Journal of Applied Physics
Verified
Journal Article
Closed access
SHS. Hammersley
S. Hammersley
DWD. Watson-Parris
D. Watson-Parris
PDP. Dawson
P. Dawson
MGM. J. Godfrey
M. J. Godfrey
TBT. J. Badcock
T. J. Badcock
CHC. J. Humphreys
C. J. Humphreys
There is a great deal of interest in the underlying causes of efficiency droop in InGaN/GaN quantum well light emitting diodes, with several physical mechanisms being put forward to explain the phenomenon. In this paper we report on the observation of a reduction in the localization induced S-shape temperature dependence of the peak photoluminescence energy with increasing excitation power density. This S-shape dependence is a key fingerprint of carrier localization. Over the range of excitation power density where the depth of the S shape is reduced, we also observe a reduction in the integrated photoluminescence intensity per unit excitation power, i.e., efficiency droop. Hence, the onset of efficiency droop occurs at the same carrier density as the onset of carrier delocalization. We correlate these experimental results with the predictions of a theoretical model of the effects of carrier localization due to local variations in the concentration of the randomly distributed In atoms on the optical properties of InGaN/GaN quantum wells. On the basis of this comparison of theory with experiment we attribute the reduction in the S-shape temperature dependence to the saturation of the available localized states. We propose that this saturation of the localized states is a contributory factor to efficiency droop whereby nonlocalized carriers recombine non-radiatively.

28 September 2015 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
SHS. Hammersley
S. Hammersley
MKM. J. Kappers
M. J. Kappers
FMF. C.-P. Massabuau
F. C.-P. Massabuau
SSS.-L. Sahonta
S.-L. Sahonta
PDP. Dawson
P. Dawson
CHC. J. Humphreys
C. J. Humphreys
InGaN-based light emitting diodes and multiple quantum wells designed to emit in the green spectral region exhibit, in general, lower internal quantum efficiencies than their blue-emitting counter parts, a phenomenon referred to as the “green gap.” One of the main differences between green-emitting and blue-emitting samples is that the quantum well growth temperature is lower for structures designed to emit at longer wavelengths, in order to reduce the effects of In desorption. In this paper, we report on the impact of the quantum well growth temperature on the optical properties of InGaN/GaN multiple quantum wells designed to emit at 460 nm and 530 nm. It was found that for both sets of samples increasing the temperature at which the InGaN quantum well was grown, while maintaining the same indium composition, led to an increase in the internal quantum efficiency measured at 300 K. These increases in internal quantum efficiency are shown to be due reductions in the non-radiative recombination rate which we attribute to reductions in point defect incorporation.

10 May 2018 in Journal of Applied Physics
Verified
Journal Article
Open access
PDF file
SCS. A. Church
S. A. Church
SHS. Hammersley
S. Hammersley
PMP. W. Mitchell
P. W. Mitchell
MKM. J. Kappers
M. J. Kappers
LLL. Y. Lee
L. Y. Lee
PDP. Dawson
P. Dawson
The photoluminescence spectra of a zincblende GaN epilayer grown via metal-organic chemical vapour deposition upon 3C-SiC/Si (001) substrates were investigated. Of particular interest was a broad emission band centered at 3.4 eV, with a FWHM of 200 meV, which extends above the bandgap of both zincblende and wurtzite GaN. Photoluminescence excitation measurements show that this band is associated with an absorption edge centered at 3.6 eV. Photoluminescence time decays for the band are monoexponential, with lifetimes that reduce from 0.67 ns to 0.15 ns as the recombination energy increases. TEM measurements show no evidence of wurtzite GaN inclusions which are typically used to explain emission in this energy range. However, dense stacking fault bunches are present in the epilayers. A model for the band alignment at the stacking faults was developed to explain this emission band, showing how both electrons and holes can be confined adjacent to stacking faults. Different stacking fault separations can change the carrier confinement energies sufficiently to explain the width of the emission band, and change the carrier wavefunction overlap to account for the variation in decay time.

20 June 2011 in physica status solidi (c)
Verified
Journal Article
Closed access
PDF file
SHS. Hammersley
S. Hammersley
TBT. J. Badcock
T. J. Badcock
DWD. Watson‐Parris
D. Watson‐Parris
MGM. J. Godfrey
M. J. Godfrey
PDP. Dawson
P. Dawson
CHC. J. Humphreys
C. J. Humphreys

5 February 2016 in Journal of Applied Physics
Verified
Journal Article
Open access
PDF file
MDM. J. Davies
M. J. Davies
SHS. Hammersley
S. Hammersley
FMF. C.-P. Massabuau
F. C.-P. Massabuau
PDP. Dawson
P. Dawson
RORachel Oliver
Rachel Oliver
CHColin Humphreys
Colin Humphreys
In this paper, we report on a detailed spectroscopic study of the optical properties of InGaN/GaN multiple quantum well structures, both with and without a Si-doped InGaN prelayer. In photoluminescence and photoluminescence excitation spectroscopy, a 2nd emission band, occurring at a higher energy, was identified in the spectrum of the multiple quantum well structure containing the InGaN prelayer, originating from the first quantum well in the stack. Band structure calculations revealed that a reduction in the resultant electric field occurred in the quantum well immediately adjacent to the InGaN prelayer, therefore leading to a reduction in the strength of the quantum confined Stark effect in this quantum well. The partial suppression of the quantum confined Stark effect in this quantum well led to a modified (higher) emission energy and increased radiative recombination rate. Therefore, we ascribed the origin of the high energy emission band to recombination from the 1st quantum well in the structure. Study of the temperature dependent recombination dynamics of both samples showed that the decay time measured across the spectrum was strongly influenced by the 1st quantum well in the stack (in the sample containing the prelayer) leading to a shorter average room temperature lifetime in this sample. The room temperature internal quantum efficiency of the prelayer containing sample was found to be higher than the reference sample (36% compared to 25%) which was thus attributed to the faster radiative recombination rate of the 1st quantum well providing a recombination pathway that is more competitive with non-radiative recombination processes.

23 April 2019 in Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
FMFabien C-P Massabuau
Fabien C-P Massabuau
MHM. K. Horton
M. K. Horton
EPE. Pearce
E. Pearce
SHS. Hammersley
S. Hammersley
PCP. Chen
P. Chen
RORachel Oliver
Rachel Oliver
Threading dislocations in thick layers of InxGa1−xN (5% < x < 15%) have been investigated by means of cathodoluminescence, time-resolved cathodoluminescence, and molecular dynamics. We show that indium atoms segregate near dislocations in all the samples. This promotes the formation of In-N-In chains and atomic condensates, which localize carriers and hinder nonradiative recombination at dislocations. We note, however, that the dark halo surrounding the dislocations in the cathodoluminescence image becomes increasingly pronounced as the indium fraction of the sample increases. Using transmission electron microscopy, we attribute the dark halo to a region of lower indium content formed below the facet of the V-shaped pit that terminates the dislocation in low composition samples (x < 12%). For x > 12%, the facets of the V-defect featured dislocation bundles instead of the low indium fraction region. In this sample, the origin of the dark halo may relate to a compound effect of the dislocation bundles, of a variation of surface potential, and perhaps, of an increase in carrier diffusion length.