The influences of cooling rate and initial composition on solidification path, microstructure and hardness of Al-Cu-Si alloys were investigated. The results indicate that the solidification paths of alloys Al-3.7Cu-6.5Si, Al-5.2Cu-2.6Si and Al-15.1Cu-6.2Si were (L + α-Al)→(L + α-Al+ β-Si)→(L + α-Al+ β-Si+ θ-Al2Cu), and the solidification paths of alloys Al-4.6Cu-0.9Si, Al-24.2Cu-3.9Si and Al-26.9Cu-2.1Si were (L + α-Al)→(L + α-Al+ θ-Al2Cu)→(L + α-Al+ β-Si+ θ-Al2Cu). Furthermore, it is found that the further the initial compositions from the binary eutectic trough and the slower the cooling rate was, the second dendrite arm spacing was larger and the volume percent of phase θ-Al2Cu was fewer, and then influence the hardness. There were three kinds of (α-Al+ θ-Al2Cu) binary eutectic, two kinds of (α-Al+ β-Si+ θ-Al2Cu) ternary eutectic and one kind of (α-Al+ β-Si) binary eutectic morphologies existed in the solidification specimens.
25 October 2019 in Journal of Materials Engineering and Performance