14 May 2021 in Journal of Physics: Condensed Matter
Magnetoelectric (ME) effect is a type of cross-coupling between unconjugated physical quantities, such as the interplay between magnetization and electric field. The ME effect requires simultaneous breaking of spatial and time inversion symmetries, and it sometimes appears in specific antiferromagnetic (AFM) insulators. In recent years, there has been a growing interest for applying the ME effect to spintronic devices, where the effect is utilized as an input method for the digital information. In this article, we review the recent progress of this scheme mainly based on our own achievements. We particularly focus on several fundamental issues, including the ME control of the AFM domain state, which is detectable through the perpendicular exchange bias polarity. The progress made in understanding the switching mechanism, interpretation of the switching energy, switching dynamics, and finally, the future prospects are included.
1 December 2013 in Applied Physics Express
We found the regeneration of perpendicular exchange bias at high temperature in the Pt-capping/Co/Pt-spacer/?-Cr2O3/Pt-buffer thin film with an ultrathin (0.2 nm) Pt-spacer layer after the disappearance at low temperature. Abrupt changes in the coercivity accompany the abrupt disappearance and regeneration of exchange bias. The direction of the regenerated exchange bias could be reversed by altering the ferromagnetic spin orientation during temperature rise. The exchange bias did not regenerate when the Pt spacer layer was grown at a slow growth rate, suggesting that the growth mode of Pt on the ?-Cr2O3 layer affects the regeneration feature.
31 October 2022 in Applied Physics Letters
Increase in the Néel temperature (TN) of the 10-nm thick Cr2O3(0001) thin films by the lattice strain was experimentally investigated. TN was determined based on the zero-offset anomalous Hall measurements for the Pt/Cr2O3/Pt epitaxial trilayer. The lattice strain was altered by the Pt buffer layer thickness and was evaluated by the lattice parameters. TN was increased from 241.5 to 260.0 K by varying the Pt buffer layer thickness from 0 to 20 nm. For the film without the Pt buffer layer, the apparent critical exponent near TN increased suggesting the distribution of TN due to the inhomogeneous strain. The TN value was weakly correlated with the axial ratio c/a and the lattice volume of the Cr2O3 layer V; TN increases with decreasing c/a or increasing V. The increase in TN by the reduction in c/a (or by increasing V) implies that the exchange coupling between the nearest neighbor Cr3+ spins has the significant role in the strain effect.
10 July 2023 in Applied Physics Letters
Antiferromagnet does not show the net magnetization, whereas the finite uncompensated moment can residue at the surface. On the surface of the magnetoelectric antiferromagnet, the finite boundary magnetization can acquire the magnetic response. In this paper, we address the magnetic response of the boundary magnetization in the Pt/magnetoelectric Cr2O3/Pt epitaxial trilayer based on the anomalous Hall effect (AHE) and the soft x-ray magnetic circular dichroism (XMCD). Decreasing the Cr2O3 thickness down to 15 nm, the film acquired the magnetic responsiveness, which manifested as the rectangular hysteresis in the magnetic field dependence of the AHE. The sizable XMCD intensity and the rectangular magnetic field dependence of the XMCD intensity revealed that the magnetic response was attributed to the interfacial Cr moment. The detailed investigation of AHE and XMCD revealed that the domain wall motion dominated the reversal process of the boundary magnetization, which was directly visualized by the scanning XMCD microscope.
28 December 2023 in Journal of Physics: Condensed Matter
We systematically investigate the long- and short-range chemical order, lattice volume, and spontaneous magnetization in single-crystalline Fe0.6Al0.4 compound thin films. The vapor-quenching method based on a molecular beam epitaxy technique is utilized to fabricate the single-crystalline Fe0.6Al0.4 compound with the different B2 long-range order parameter S. S was varied by the deposition temperature T d, and it increases with increasing T d. The lattice volume V decreased with increasing T d, while the tetragonal distortion, ∼4%, due to epitaxial strain were observed. The changes in S and V were accompanied with the change in the magnetic moment per Fe, μ Fe. μ Fe showed the monotonic decrease as a function of S whereas μ Fe monotonically increases with V. With considering tetragonal distortion, μ Fe–V relationship has a good agreement with the previous reports. The μ Fe–S relationship showed the steep decrease of μ Fe around S∼ 0.6. In contrast to μ Fe–V relationship, μ Fe–S relationship does not match only from ours to previous studies but also among other reports. It implies the statistical number of the nearest-neighbor Fe–Fe bonds, i.e. S, cannot be an enough explanatory parameter. To clarify the structural origin of change in μ Fe, the short-range order (SRO) parameter inferred from the analysis of superlattice diffractions were introduced. They showed the clear difference for the films with high and low μ Fe. The results suggest that the transition from the long- to the SRO state plays the significant role on μ Fe.