2 June 2026 in SSRN Electronic Journal
Understanding stress evolution in diamond/SiC heterostructures is critical for high-power electronic applications, yet the thickness-dependent stress transition and its thermal behavior remain underexplored. Here, a synergistic approach combining temperature-dependent Raman spectroscopy and finite element simulation to systematically investigate the stress evolution of diamond films (5–280 µm) on 4H-SiC substrates from 27 °C to 600 °C is adopted. A distinct tensile-to-compressive stress transition is observed within the critical thickness range of 100–200 µm. Thin films (5 µm and 100 µm) are dominated by tensile stress (e.g., D100 exhibits 0.50 GPa tensile stress at 27 °C), whereas thick films (200 µm and 280 µm) show compressive stress (e.g., D200 presents 0.23 GPa compressive stress). Raising the temperature to 600 °C relieves thermal stress, with reduction rates at the center and edge of the 280 µm-thick film reaching 45% and 86%, respectively. Spatial stress distribution reveals that center stress is higher than edge stress, with the difference widening with increasing temperature and film thickness. Films exhibit a stress-temperature trend of first increasing then decreasing, while the edge of the thickest film remains compressive across the entire range. FEM results agree well with thin-film experiments but show notable deviations for thick films. The optimal diamond/SiC thickness ratio is identified as 1:5–2:5, enabling low-stress diamond films by regulating the tensile-to-compressive stress transition. This work clarifies the stress evolution law of diamond/SiC heterostructures, and provides a practical design pathway towards low-stress, thickness-tailored diamond/SiC composites for next-generation high-power electronic and thermal management systems.