18 October 2019 in Energy & Environmental Science
Understanding the fundamentals of iridium degradation during the oxygen evolution reaction is of importance for the development of efficient and durable water electrolysis systems. The degradation mechanism is complex and it is under intense discussion whether the oxygen molecule can be directly released from the oxide lattice. Here, we define the extent of lattice oxygen participation in the oxygen evolution and associated degradation of rutile and hydrous iridium oxide catalysts, and correlate this mechanism with the atomic-scale structures of the catalytic surfaces. We combine isotope labelling with atom probe tomography, online electrochemical and inductively coupled plasma mass spectrometry. Our data reveal that, unlike rutile IrO2, Ir hydrous oxide contains –IrIIIOOH species which directly contribute to the oxygen evolution from the lattice. This oxygen evolution mechanism results in faster degradation and dissolution of Ir. In addition, near surface bulk regions of hydrous oxide are involved in the oxygen catalysis and dissolution, while only the topmost atomic layers of rutile IrO2 participate in both reactions. Overall our data provide a contribution to the fundamental understanding of the exceptional stability of Ir-oxides towards the oxygen evolution reaction. The proposed approach to a quantitative assessment of the degree of lattice oxygen participation in the oxygen evolution reaction can be further applied to other oxide catalyst systems.
1 June 2021 in Acta Materialia
4 June 2020 in The Journal of Physical Chemistry Letters
The development of efficient acidic water electrolyzers relies on understanding dynamic changes of the Ir-based catalytic surfaces during the oxygen evolution reaction (OER). Such changes include degradation, oxidation and amorphization processes, each of which somehow affect the material’s catalytic performance and durability. Some mechanisms involve the release of oxygen atoms from the oxide’s lattice, the extent of which is determined by the structure of the catalyst. Whilst the stability of hydrous Ir-oxides suffers from the active participation of lattice oxygen atoms in the OER, rutile IrO2 is more stable and the lattice oxygen involvement is still under debate due to the insufficient sensitivity of commonly used online electrochemical mass spectrometry. Here, we revisit the case of rutile IrO2 at the atomic scale by a combination of isotope-labelling and atom probe tomography, and reveal the exchange of oxygen atoms between the oxide lattice and water. Our approach enables direct visualization of the electrochemically active volume of the catalysts and allows for the estimation of an oxygen exchange rate during the OER which is discussed in view of surface restructuring and subsequent degradation. Our work presents an unprecedented opportunity to quantitatively assess the exchange of surface species during an electrochemical reaction, relevant for the optimization of the long-term stability of catalytic systems.
18 November 2016 in Energy & Fuels
The pore space of shales and mudrocks ranges from molecular dimensions to micrometers in length scale. This leads to great variation in spatial characteristics across many orders of magnitude, which poses a challenge for the determination of a representative microscopic pore network for such systems. Standard characterization techniques generally provide volume-averaged properties while high-resolution imaging techniques do not assess a representative range of pore sizes because of limitations in the spatial resolution over the field of view. Due to this complexity, open questions remain regarding the role of the pore network in retention and transport processes, which in turn control oil and gas production. Volume-averaged but spatially resolved information is obtained for pores of size from 2 to 150 nm by applying scanning small- and wide-angle X-ray scattering (SAXS and WAXS) microscopy. Scattering patterns are collected in a scanning microscopy mode, such that microvoxels are sampled sequentially, over a total of 2 × 2 mm2 raster area on specifically prepared thin sections with a thickness of 10–30 μm. Spatially resolved variations of porosity, pore-size distribution, orientation, as well as mineralogy are derived simultaneously. Aiming at a full characterization of the shale pore network, the measurements and subsequent matrix porosity analysis are integrated in a multiscale imaging workflow involving FIB-SEM, SEM, and μ-CT analysis.
23 August 2019 in Contributions to Mineralogy and Petrology
5 February 2021 in Contributions to Mineralogy and Petrology