3 October 2024 in IEEE Journal of Photovoltaics
PBPierre-Olivier Bouchard
The thermal expansion behavior of polymers is a crucial property for manufacturing photovoltaic (PV) modules. The thermal expansion mismatch between the different module components induces residual stresses in the structure after manufacturing. Some of them are located at the interface between materials, leading to delamination and reliability issues during the PV module lifetime. For tandem applications, the thermal expansion mismatch is also an issue since it leads to the separation between the bottom and top cells. In this article, the thermal expansion behavior of a thermoplastic polyolefin (TPO) encapsulant used in the PV industry is assessed by stereo digital image correlation. This contactless method measures the thermal expansion in the two directions of the polymer thin film. The method is accurate enough to capture transition phases of the material, namely the crystallites fusion and formation. The thermal expansion behavior of the TPO thin film is shown to be anisotropic and dependent on its thermal history. The material contracts when heated, both after manufacturing and after aging; this has not yet been investigated. The aging temperature has an influence on the thermal contraction temperature but does not erase the shrinking behavior. The thermal expansion behavior is explained by a microstructural approach. The microstructure is investigated by differential scanning calorimetry. After crystallites melting, the molecular mobility and residual internal stresses account for the observed shrinking behavior. This behavior may affect the reliability of PV modules through delamination, cells cracks, or separation of the top and bottom cells.
9 January 2023 in EPJ Photovoltaics
Since the renewable energy thrive, performances and lifetime of photovoltaic (PV) modules have been one of the big international concern. The mechanical bonding between the different components and the materials' choice can significantly improve both performances and lifetime of PV modules. The manufacturing process plays also a significant part in the modules lifetime [G. Oreski, B. Ottersböck, A. Omazic, Degradation Processes and Mechanisms of Encapsulants, in Durability and Reliability of Polymers and Other Materials in Photovoltaic Modules (Elsevier, 2019), pp. 135–152]. This work deals with the controlled cooling part of the manufacturing process. The aim is to characterize its influence on an encapsulant properties, and its influences on modules degradation. This work is a part of improving both performances and lifetime of PV modules. First, the work focuses on describing the real temperature seen by a thermoplastic polyolefin encapsulant during the lamination process. A multi-chamber R&D laminator is used and studied in order to better know the industrial equipment. Results show that the cooling process reduces the time to cool down by a factor of ∼5 compared to natural air convection. Secondly, the material's micro-structure is analysed by Differential Scanning Calorimetry (DSC). The impact of the process is quantified. It does have an influence on the encapsulant crystallites' size distribution without modifying the total crystallinity. Thirdly, the impact of the cooling process on optical properties is investigated. Using spectrophotometry and haze-metry optical characterization, coupled with a known light spectrum, the light intensity coming out from the material is analysed. Results show that the cooling process does not have any influence on transmittance nor reflectance. However, a 34% reduction in the haze factor is recorded when using the industrial laminator cooling process. Fourthly, mechanical bond strength between glass and encapsulant is characterized over ageing. Normalized 10 mm width strips are used to estimate the bond strength. It demonstrates that applying pressure during cooling does not influence the bond strength between glass and encapsulant after 1000 h of damp heat ageing. Finally, impact of the cooling process over ageing on PV modules is discussed. Two accelerating ageing methods, 300 Thermal Cycles and 1000 h damp heat, are used to speed up ageing processes. The electrical components of the PV modules are analysed and used to assess the modules' degradation. Modules manufactured with the cooling process are more sensitive to damp heat after 500 h than modules cooled by natural convection. No significant differences were found in thermal cycling ageing.
26 July 2025 in Solar Energy
PBPierre-Olivier Bouchard