Tong Zhao

Tong Zhao

Auto-generated profile, based on publicly available information

Tong Zhao

Shanghai Institute of Technical Physics , Shanghai , China

Research Focus & Metrics

Academic Career Length

25Years (2002-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
8 November 2002 in Nanotechnology
Verified
Journal Article
Closed access
HWH M Wu
H M Wu
YSY L Song
Y L Song
TZT Zhao
T Zhao
LJL Jiang
L Jiang
HLH W Liu
H W Liu
HGH J Gao
H J Gao

15 September 2023 in Advanced Engineering Materials
Verified
Journal Article
Closed access
TZTong Zhao
Tong Zhao
DMDefeng Mo
Defeng Mo
XSXinmin Shi
Xinmin Shi
WSWen Sun
Wen Sun
XLXue Li
Xue Li
HGHaimei Gong
Haimei Gong

29 November 2022 in Materials Testing
Verified
Journal Article
Closed access
DMDefeng Mo
Defeng Mo
LYLiquan Yu
Liquan Yu
XSXinmin Shi
Xinmin Shi
TZTong Zhao
Tong Zhao
XLXue Li
Xue Li
HGHaimei Gong
Haimei Gong
Electron beam welding of TC4 titanium alloy and 4J29 Kovar alloy was performed by using different thicknesses of silver interlayers. The microstructure and the composition of welded joints were characterized by scanning electron microscopy, X-ray diffraction, and energy-dipersive spectrometry. The mechanical properties of welded joints were evaluated by tensile strength tests. The results indicated that Ag thickness has great effects on the weld appearance, microstructure, and mechanical properties of electron beam-welded joints. In case of 0.3 and 0.4 mm thickness of Ag interlayers, a considerable part of 4J29 and TC4 melts and a large amount of Fe, Ti, and Ni elements diffuse into the molten pool forming intermetallic compounds (IMCs) such as TiFe2, NiTi, and FeTi. In case of 0.6 mm thickness of Ag interlayer, the welded joint exhibits brazing characteristics with little IMCs near the fusion line of 4J29 Kovar alloy side. When the thickness of the Ag interlayer increases to 0.8 mm, the diffusion of Ti and Fe elements is completely inhibited by Ag. As the thickness of the Ag interlayer increases from 0.3 to 0.8 mm, the tensile strength of the welded sample shows a phenomenon that first rises and then falls, and the largest tensile strength is 243 MPa.

11 January 2024 in Materials Testing
Verified
Journal Article
Closed access
TZTong Zhao
Tong Zhao
DMDefeng Mo
Defeng Mo
XLXue Li
Xue Li
HGHaimei Gong
Haimei Gong
Si3N4 and Invar alloy brazed joints were achieved using two types of Ag-based interlayers: a Ag–Cu–In–Ti foil and a Ag–Cu–In–Ti/Cu/Ag–Cu multi-interlayer. The results showed that when only using a single Ag–Cu–In–Ti filler, the wave-shaped Fe2Ti + Ni3Ti intermetallic compounds are concentrated in the middle of the brazing seam. When adding Cu as the interlayer, the dissolution of the Cu interlayer formed a large number of Cu(s,s) blocks of different sizes in the brazing seam, which hindered the concentrated distribution of Fe2Ti + Ni3Ti intermetallic compounds in the brazing seam. As a result, Fe2Ti and Ni3Ti were dispersedly distributed in the brazing seam, increasing the shear strength of the brazed joint. The shear strength of brazed joints was increased by 82 % compared to joints brazed with a single Ag–Cu–In–Ti filler when the Cu interlayer was added.