Reflective cracking is one of the major forms of deterioration in pavements and is very common when hot-mix asphalt (HMA) overlays are constructed over a base with discontinuities in its surface. This issue has not received proper attention compared with classical fatigue cracking. However, it is a major concern during the selection of asphalt mixture surface courses for pavements with an underlying cracked base. This work identified the most appropriate testing device for investigating the resistance of asphalt mixtures to reflective cracking in the laboratory. An in-depth review of the available literature was conducted and 17 reflective cracking testing devices were evaluated, among which best three were chosen based on their availability, ease of use, variability, repeatability of the test results, and field validation. It was concluded that the Hamburg wheel tracking tester (HWTT), the wheel reflective cracking (WRC) apparatus, and the upgraded Texas Transportation Institute (TTI) overlay tester are the best available devices to examine resistance to reflective cracking in the laboratory.
Human activities significantly contribution to the yearly generated plastic wastes. Moreover, the enormous increase in face masks and face shields caused by the emergence of the COVID-19 pandemic has doubled the generated plastic wastes. Although there is an added benefit of using plastic waste in construction, the cost associated with their application, specifically the face mask, has not been addressed. This paper presents a simplified and rapid estimation of the cost associated with the collection, processing, and application of face masks in hot-mix asphalt (HMA) pavements. Two scenarios, mask modified asphalt pavement and conventional asphalt pavement, are considered. The total cost is based on market price and prices from waste management facilities and plastic processing companies. Life Cycle Cost Analysis (LCCA) is used to evaluate the long-term costs of mask modified asphalt pavement and conventional asphalt pavement. Results show that no significant difference in initial total cost between the two scenarios for pavement sections with lengths less than 500m and the number of lanes less than 6. The difference in total cost begins with lengths greater than 500 m for 5 and 6 Lanes. Despite the higher initial costs for the mask modified asphalt pavement, the LCCA shows that there is a 29% maintenance cost reduction over the 40 years life cycle of the asphalt pavement. The use of LCCA shows the benefit of the selection of the most cost-effective strategy and how the use of mask modified asphalt pavement over the conventional asphalt pavement can save money over the life cycle of the asphalt and improve rutting and stiffens.
1 January 2020 in Journal of Materials in Civil Engineering
Short-term oven aging (STOA) is used in current practice to simulate typical aging of asphalt mixtures during plant production and field construction. This study compares the volumetrics and performance of laboratory-produced asphalt mixtures and corresponding plant-produced mixtures to examine whether STOA simulates plant short-term aging. Eight plant-produced mixtures with varying levels of binder performance grade, binder content, filler content, and traffic design levels were tested for rutting and cracking resistance using Hamburg wheel-tracking (HWT) and semicircular bending (SCB) tests, respectively. The eight mixtures were duplicated in the laboratory and subjected to 2 h of reheating and 2 h of oven aging before testing. The eight lab-produced mixtures had comparable volumetric properties to the plant-produced mixtures, and the performance results showed a relatively high level of equality between plant- and lab-produced mixtures even when the properties of their extracted and recovered binders at high and intermediate temperatures are found to be significantly different. Based on the findings of this study, the use of the outlined STOA procedure is considered sufficient to represent standard plant production aging.