Dmitrii Evgenyevich Cherepanov

Dmitrii Evgenyevich Cherepanov

Auto-generated profile, based on publicly available information

Dmitrii Evgenyevich Cherepanov

Budker Institute of Nuclear Physics, Siberian Branch, Russian Academy of Sciences, Novosibirsk, Russia

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
27 August 2023 in Nuclear Materials and Energy
Verified
Journal Article
Open access
DCD.E. Cherepanov
D.E. Cherepanov
LVL.N. Vyacheslavov
L.N. Vyacheslavov
VPV.A. Popov
V.A. Popov
GRG.A. Ryzhkov
G.A. Ryzhkov
AKA.A. Kasatov
A.A. Kasatov
ASAndrey Shoshin
Andrey Shoshin

1 December 2024 in Physics of Atomic Nuclei
Verified
Journal Article
Closed access
PDF file
DCD. E. Cherepanov
D. E. Cherepanov
ABA. V. Burdakov
A. V. Burdakov
LVL. N. Vyacheslavov
L. N. Vyacheslavov
SKS. R. Kazantsev
S. R. Kazantsev
IKI. V. Kandaurov
I. V. Kandaurov
ASAndrey Shoshin
Andrey Shoshin
The boron carbide coatings deposited on tungsten using three methods have been tested by pulsed heating, which is expected on the first wall and in the divertor zone of the ITER tokamak. The deposition methods chosen were detonation spraying, atmospheric plasma spraying, and electron beam synthesis. The experiments revealed that the best resistance to pulsed heating is demonstrated by coatings applied using detonation and atmospheric plasma spraying methods.

1 November 2025 in Plasma Science and Technology
Verified
Journal Article
Closed access
DCDmitrii Cherepanov
Dmitrii Cherepanov
GRGeorgii Ryzhkov
Georgii Ryzhkov
LVLeonid Vyacheslavov
Leonid Vyacheslavov
AKAlexandr Kasatov
Alexandr Kasatov
IBIgor Batraev
Igor Batraev
IKIgor Kandaurov
Igor Kandaurov
A boron carbide (B 4 C) coating, deposited on tungsten using the detonation spraying method, was tested under high pulse number transient heat loads expected during the ITER tokamak H-mode operation. The heat loads were relevant to those caused by edge localized modes (ELMs) and mitigated disruptions. The results showed that in the case of ELM-like heating expected in the first wall zone of the ITER tokamak, the coating is capable to withstand pulses before detachment from the substrate. In the case of thermal shocks with more intense heating by mitigated plasma disruptions or ELM-like heating in the divertor zone, the coating detached only after several pulses. The results of the work show that transient heat load is a serious factor limiting the use of B 4 C as a plasma-facing material. The use of such ceramic coatings requires the development of ELM and disruption mitigation systems, as well as in situ coating renewal methods.

1 March 2021 in Nuclear Materials and Energy
Verified
Journal Article
Open access
DCD.E. Cherepanov
D.E. Cherepanov
AAA.S. Arakcheev
A.S. Arakcheev
ABA.V. Burdakov
A.V. Burdakov
IKI.V. Kandaurov
I.V. Kandaurov
AKA.A. Kasatov
A.A. Kasatov
LVL.N. Vyacheslavov
L.N. Vyacheslavov

9 October 2025 in Plasma Science and Technology
Verified
Journal Article
Closed access
DCDmitrii Evgenyevich Cherepanov
Dmitrii Evgenyevich Cherepanov
MGMikhail Alekseevich Golosov
Mikhail Alekseevich Golosov
LVLeonid Vyacheslavov
Leonid Vyacheslavov
NBNatalia Ivanovna Baklanova
Natalia Ivanovna Baklanova
GRGeorgii Ryzhkov
Georgii Ryzhkov
ABAlexandr Vladimirovich Burdakov
Alexandr Vladimirovich Burdakov
Studies were carried out on the thermally induced erosion of silicon carbide as a result of pulsed infrared laser heating, simulating transient heat loads expected in the ITER tokamak divertor zone (laser pulse duration: ∼ 0.5 ms). The critical parameters of pulsed heating that the material can withstand before the onset of erosion with loss of substance were determined. The experimentally observed damage threshold of hot-pressed silicon carbide under thermal shock of submillisecond duration corresponds to a temperature of about 1320±80 K, while a heat flux factor is about 23.9±1.6 MJ·m-2·s-0.5 (the sample was initially at room temperature). This result is relevant for surfaces with low roughness (Ra ≈ 1.1 μm, Rz ≈ 5.3 μm). An increase in surface roughness leads to a decrease in the resistance of ceramics to pulsed heating. For rough surface (Ra ≈ 1.7 μm, Rz ≈ 9.3 μm) critical temperature of about 790±50 K and heat flux factor of about 11.6±0.8 MJ·m-2·s-0.5 were obtained. Thus, silicon carbide exhibits excellent resistance to transient heat loads as promising plasma-facing material, especially in the case of reduced surface roughness.

28 November 2025 in Fusion Engineering and Design
Verified
Journal Article
Closed access
GRG.A. Ryzhkov
G.A. Ryzhkov
DCD.E. Cherepanov
D.E. Cherepanov
MGM.A. Golosov
M.A. Golosov
AKA.A. Kasatov
A.A. Kasatov
VPV.A. Popov
V.A. Popov
GLG.G. Lazareva
G.G. Lazareva