High-entropy alloys (HEAs) provide a broad compositional space for tuning phase stability and surface durability. CoCrFeNiMnx (x = 0.5, 1.0, 1.5, and 2.0) alloys were fabricated by vacuum arc melting and characterized by X-ray diffraction (XRD), optical microscopy (OM), scanning electron microscopy with energy-dispersive spectroscopy (SEM/EDS), microhardness testing, electrochemical testing in 3.5 wt.% NaCl, and X-ray photoelectron spectroscopy (XPS). Density functional theory (DFT) calculations and first-principles molecular dynamics were further employed to analyze the Mn-dependent electronic structure and oxygen–metal bonding. The XRD results indicate a transition from a single FCC solid solution at x ≤ 1.0 to an FCC + BCC constitution at x ≥ 1.5. With increasing Mn, microstructures evolve from coarse dendrites toward higher fractions of equiaxed grains. Hardness decreases from 163.6 HV (x = 0.5) to 125.1 HV (x = 1.0) and then increases to 162.6 HV (x = 2.0), indicating competing solid-solution and phase/segregation effects. Electrochemical measurements show enhanced corrosion resistance with Mn addition; the x = 2.0 alloy exhibits the lowest fitted corrosion current density (icorr = 0.3482 × 10−6 μA·cm−2) and the most stable passivation response. XPS reveals passive films dominated by Fe2O3 together with Mn3+ oxides, whose synergistic formation promotes a denser barrier layer. DFT predicts a monotonic decrease in Fermi level and a narrowed conduction band range as Mn increases, consistent with reduced electron transfer activity during anodic dissolution. Interfacial simulations show that O preferentially bonds with Cr and Mn, while Ni–O bonds have the lowest estimated rupture barrier, rationalizing a tendency toward localized corrosion at Ni-associated sites.
The effects of preheating temperature on the microstructural evolution and mechanical properties of low-activity martensitic steel welded joints were investigated, with emphasis on the relationship between preheating temperature, δ-ferrite content, and impact energy. Preheating temperature ranged from 150 °C to 300 °C. Optical microscopy and TEM were used for microstructural characterization, and tensile and impact tests were conducted to evaluate mechanical properties. The results showed that preheating temperature influenced the retained δ-ferrite content in the weld metal, whereas its effect on the heat-affected-zone microstructure was comparatively limited. The δ-ferrite fraction exhibited a non-monotonic dependence on preheating temperature, reaching a minimum of 2.76% in the filler weld pass at 250 °C. As the δ-ferrite fraction increased to approximately 13.27% at 150 °C, the average impact energy of the weld metal decreased from 47.37 J at 250 °C to 34.57 J at 150 °C. Impact fracture analysis revealed preferential crack propagation along δ ferrite/martensite interfaces and through δ-ferrite grains. An increase in the δ-ferrite fraction may promote the formation of interconnected ferrite networks, thereby facilitating crack propagation and reducing the impact toughness of the weld metal.