With further development of oil and gas resources, corrosion environment of gathering lines became more serious. Designers must consider H2S cracking and H2S corrosion, especially in oil and gas fields with H2S and CO2 rich gas. In this severe, sour environment, carbon steel with inhibition was not ineffective or infeasible in combating corrosion and cracking. Nickel-based, corrosion-resistant alloy (CRA) could resist corrosion, but its expensive price often makes it difficult to provide the economic justification for its use. Therefore, bimetallic-lined pipe, which has a liner pipe made of CRA and an outer pipe made of low-cost steel, might be an effective solution to the corrosion problem. Application of bimetallic-lined pipe in oil and gas field environments has been a topic of signification interest, involving both performance and economic questions. This paper analyzes four anti-corrosion measures: (1) carbon steel with corrosion allowance, (2) carbon steel with inhibitor, (3) CRA and bimetallic-lined pipe from technical and economic perspectives. The results showed that bimetallic-lined pipe had the greatest advantages in technology and economics. So far, however, bimetallic-lined pipe has not been used as gathering lines for sour service in China. There are still many questions to deal with. The paper describes three primary questions and puts forward some proposed solutions, including: (1) material selection and performance control; (2) manufacturing technique of pipe fitting; and (3) assessment of girth weld procedure. Ultimately, the obtained conclusion is that bimetallic-lined pipe owned a higher performance price ratio and must be widely used in highly corrosive oil and gas fields.
As the main source gas reservoir of the West to East Gas Pipeline Project, the Yaha Gas Condensate Field was a condensate gas reservoir located in the Tarim basin in the northwestern China that started to supply gas in 2000. The gas produced by the field contained about 0.7–1.3 volume percent CO2 and Clion concentration as much as 116,000ppm. Initially, 16Mn steel was adopted to construct the pipelines. By May of 2006, there were as many as fifty failures. The investigations on corrosion of flow line at simulated internal service conditions found the high corrosion rate was due to the multiphase flow induced erosion and CO2 corrosion. Considering severe corrosion environments in the Yaha Gas Condensate Field, bimetallic lined pipes, with a liner pipes made of CRA and an outer pipes made of low-cost steel, might be a potential anticorrosion solution. In this paper, the outcome of a comprehensive program of work to establish suitability of bimetallic lined pipe for gathering lines in Yaha Gas Condensate Field was presented. Manufacturing technique of bimetallic lined pipe, assessment of girth welding procedure, corrosion performance in the simulated condition and analysis on economics advantages of bimetal lined pipe were all discussed. Fit-for-purpose analysis showed that bimetal lined pipes could be an economic and effective solution to the corrosion problem in the Yaha Gas Condensate Field.