26 June 2010 in Journal of Materials Science
1 August 2007 in Science and Technology of Welding and Joining
This study is carried out to investigate the laser spot welds (LSWs) of advanced high strength steel sheets of 1·0 mm thickness for application to the automotive industry. Mechanical properties and failure behaviour of LSWs for transformation induced plasticity steel sheets (TRIP800) subjected to monotonic coach–peel loading are investigated by experimental and finite element (FE) simulation methods. Microstucture of LSW and fracture surfaces of the welded specimens were examined by scanning electron microscopy (SEM) to describe the microstructural features and to clarify the crack initiation mechanism respectively. Based on simulation solutions equivalent plastic strain was obtained to describe local deformation of LSW joints. Experimental results revealed a ‘plug type’ of failure mode of the circular LSW joints under ‘peel–coach’ loading condition. This type of ductile failure is the most common failure mode for spot welds used in the automotive industry. Numerical simulation of damage process was compared with experimental results and this revealed that fracture path was successfully predicted.
1 June 2022 in Materials Testing
In this study, a low-alloy steel component was manufactured using specially produced E70C-6M class of metal-cored welding wire according to AWS A5.18 standard for the WAAM process. The manufactured low-alloy steel component was first subjected to radiographic examination to detect any weld defect. Uniaxial tensile tests were conducted for the bottom, middle and upper regions. The micro-hardness tests were performed parallel to the deposition direction. The results show that microstructures varied from base metal to the face region of the WAAM component, including the bottom, middle and top sections. The bottom region showed lamellar structures; the middle and upper region presented equiaxed ferrite structure with a small amount of grain boundary pearlites and the face region displayed a mix of equiaxed and lamellar structures of ferrites. The yield and ultimate tensile strengths of the top, middle, and bottom regions exhibited similar results varying between 370 MPa and 490 MPa, respectively. In contrast, the top region showed an elongation value about 15% higher than other regions. Moreover, the yield and ultimate tensile strength for WAAM-produced component were found to be 14% and 24% lower than the multiple-pass all-weld metal of E70C-6M class of metal-cored wire.
1 December 2004 in Science and Technology of Welding and Joining
TiAl intermetallic alloys have been joined using the diffusion brazing technique with Ti insert foil metal combined with Cu, Ni or Fe foils. Defect-free joints can be fabricated successfully, no matter which kind of foil combination is used as insert metal. The interface structures of the joints were also investigated and results showed various interface structures in the joined zones. A mechanism for the development of the interface structure is proposed. It is suggested that the formation process of the liquid phase was responsible for the resulting interface structures. Post-bond heat treatment (PBHT) had no obvious effect on the interface structure of the joints because of the low diffusion coefficient of Cu, Ni and Fe in the parent material. Microhardness results showed a slight decrease in the joint area as a result of PBHT.
1 February 2008 in Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science
In the case of welded structures with cracks, a number of parameters, such as those with units of length, makes it difficult to present the results of numerical solutions in a form convenient for direct engineering applications, such as flaw assessment procedures. For centre-cracked components under tension, it is shown in the current article that an effect of crack length on the limit load can be taken into account by means of an upper bound limit load for the corresponding structure with no crack without any additional numerical treatment. Using this result, it is sufficient to find an upper bound limit load for the structure with no crack and then to apply the analytical formulae for finding the corresponding limit load for the structure of interest. Welding of some aluminium alloys for structural applications usually leads to a significantly lower strength (undermatched) weld joint. The approach proposed is used to demonstrate an effect of three-dimensional deformation on an upper bound limit load for such highly strength undermatched centre-cracked welded specimens under tension. This result can also be used in metal-forming applications where upper bound solutions are more useful than lower bound solutions.
31 December 2022 in International Journal of 3D Printing Technologies and Digital Industry
Wire-arc additive manufacturing (WAAM) is a promising method to produce many functional components in different industries. In this method, the welding wires from the feedstock are melted by arc discharge and deposited layer by layer. Other welding wires having different chemical compositions can also be added to the top of the previously deposited layer by replacing the feed wire from the stock to produce bimetallic components. This study investigated the feasibility of using robotic wire arc additive manufacturing technology to produce a bimetallic cutting tool. The bimetallic cutting tool was produced by depositing MSG 6 GZ-60 hard-facing welding wire on top of the austenitic stainless-steel wall produced with ER 316LSi solid wire. The cutting-based equipment requires an increased abrasion resistance with the combination of ductility to provide adequate tool life and performance. Thus, detailed microstructural analysis and hardness tests were conducted to understand the general microstructural characteristic of the manufactured cutting tool, including interfaces between two different materials.