Medium-entropy oxides are commonly employed as electrocatalysts for the oxygen evolution reaction (OER) in electrolysers aimed at producing sustainable hydrogen. However, their poor conductivity poses a significant obstacle to further enhancing their electrocatalytic activity. It is therefore imperative to develop stable and highly active non-precious metal electrocatalysts for the advancement of sustainable energy technologies. CeO2 is incorporated into the FeNiMnO4 medium-entropy spinel oxide system as an “electron pump” to facilitate electron transfer from FeNiMnO4 to CeO2. Benefiting from the heterogenous interface and medium-entropy system, the medium-entropy spinel oxide FeNiMnO4/CeO2 heterojunction electrocatalyst exhibits exceptional activity and stability for the alkaline OER. It requires an overpotential of 241 mV to reach the benchmark current density of 10 mA cm−2 with a lower Tafel slope of 44.8 mV dec−1. Theoretical calculations indicate that the incorporation of CeO2 effectively lowers the barriers for the potential-determining steps in the OER, and optimizes the electronic structure to facilitate the OER process. The present study demonstrates that constructing medium-entropy heterojunction materials represents a crucial approach towards developing efficient and durable OER electrocatalysts.
In this study, a NiCr/YSZ coating was applied to a γ-TiAl surface using multi-arc ion plating technology to enhance its high-temperature performance and explore the mechanisms of high-temperature oxidation and thermal corrosion. The thermal corrosion properties of the γ-TiAl matrix and NiCr/YSZ coating were investigated at 850 °C and 950 °C using a constant-temperature corrosion test in a 75% Na2SO4 + 25% NaCl mixture. The results indicate that after 100 h, the thermal corrosion weight gain of the coating samples was 70.1 mg/cm2 at 850 °C and 118.2 mg/cm2 at 950 °C. At these temperatures, sulfide formation on the surface increases, leading to a loose and porous surface. After 100 h of high-temperature corrosion at 850 °C, the primary oxidation product on the surface of the coating was tetragonal-ZrO2. At 950 °C, Y2O3, which mainly acts as a stabilizer in YSZ, reacted with Na2SO4, resulting in the continuous consumption of Y2O3. This reaction caused a substantial amount of tetragonal-ZrO2 to transform into monoclinic-ZrO2, altering the volume of the ceramic layer, which induced internal stress, crack propagation, and minor spallation. A continuous and dense internal thermally grown oxide (TGO) layer effectively impeded the diffusion of molten salt substances and oxygen, thereby significantly improving the thermal corrosion resistance of the thermal barrier coating.