30 June 2015 in Journal of the Electrochemical Society
Micro-Raman spectroscopy was used to characterize the rust formed on 1008 carbon steel exposed to marine test sites in Hawaii. Besides lepidocrocite in the outer rust layers and goethite in the inner rust layers, akaganeite was detected on all samples due to the presence of Cl− and increased in quantity in the rust layer with increasing Cl− deposition rate. The presence of Cl− did not affect the corrosion rate of carbon steel when the Cl− deposition rate was lower than a threshold of approximately 75 mg/m2/day, but significantly increased the corrosion rate when the Cl− deposition rate was higher than the threshold. This is likely due to akaganeite being a sink for Cl− by incorporating it into its tunnel structure when salt deposition is below a certain level. Once the akaganeite is saturated with Cl− and the akaganeite cannot take up any more Cl−, free Cl− can be available to accelerate corrosion at anodic sites.
1 March 2018 in Corrosion Science
1 January 2012 in Journal of the Electrochemical Society
The study of NaCl particle-induced atmospheric corrosion is facilitated by in situ Raman spectroscopic analysis through real time identification of corrosion products. Droplet formation on carbon steel by the deliquescence of pre-deposited NaCl particles that were exposed to high relative humidity (RH) (>80%), and corrosion initiation under the droplets were observed using an optical microscope. Pitting initiated within several minutes under the NaCl droplets. In situ and ex situ Raman spectra from the various rust species that formed during the corrosion process show that green rust (GR) formed close to the corrosion pit (i.e., anodic site) while lepidocrocite (γ-FeOOH) clusters precipitated outside of the GR region. A small amount of magnetite (Fe3O4) was also detected, mostly in the transitional region from GR to lepidocrocite. Upon exposure to an ambient atmosphere, GR transformed to lepidocrocite. This study confirms that the initial rust formed in NaCl particle-induced marine atmospheric corrosion of carbon steel is GR and lepidocrocite. While revealing the initiation mechanisms of NaCl particle-induced marine atmospheric corrosion of carbon steel, this study also provides insights for future studies involving wet-dry cycle exposures, which are more akin to the real atmospheric corrosion process.
1 June 2018 in Electrochimica Acta
1 January 2012 in Electrochemistry Communications
5 April 2014 in Journal of the Electrochemical Society
The characterization and corrosive effect of marine salt particles and seawater droplets that naturally deposited onto carbon steel and pure zinc that were exposed to marine test sites were studied. Most of the salt particles had diameters ranging from approximately 2–10 μm, and varied in their composition ranging from almost pure NaCl or KCl to mixtures of NaCl, KCl, CaCl2, and MgCl2. The differences in composition may depend on whether the seawater droplets dehydrate, crystallize, and fragment while airborne, or if they deposit as liquid droplets prior to crystallizing. The deposition of salt particles also decreased as the wind velocity decreased. The initial stage of marine atmospheric corrosion of the carbon steel and pure zinc induced by the salt deposition was also investigated. On the carbon steel substrate, NaCl-containing seawater droplets smaller than approximately 30 μm could not initiate corrosion even after 30 minutes of exposure; whereas, droplets larger than approximately 30 μm induced corrosion within approximately 30 minutes with lepidocrocite as the corrosion product. Corrosion initiated on the pure zinc samples under droplets of all sizes within 30 minutes. On the zinc samples, simonkollite formed in the central anodic region; whereas, hydrozincite formed in the peripheral cathodic region.