Hafsah Azfar Khan

Hafsah Azfar Khan

Auto-generated profile, based on publicly available information

Hafsah Azfar Khan

University of Ottawa

Research Focus & Metrics

Academic Career Length

3Years (2024-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
22 March 2024 in Energy
Verified
Journal Article
Closed access
HKHafsah A. Khan
Hafsah A. Khan
Muhammad TawalbehMuhammad Tawalbeh
Muhammad Tawalbeh
BABashar Aljawrneh
Bashar Aljawrneh
WAWaad Abuwatfa
Waad Abuwatfa
Amani Al-OthmanAmani Al-Othman
Amani Al-Othman
AOAbdul Ghani Olabi
Abdul Ghani Olabi

23 October 2025 in Journal of Power Sources
Verified
Journal Article
Closed access
HKHafsah A. Khan
Hafsah A. Khan
zouina Karkarzouina Karkar
zouina Karkar
MHMohamed S.E. Houache
Mohamed S.E. Houache
EBElena A. Baranova
Elena A. Baranova
Yaser Abu-LebdehYaser Abu-Lebdeh
Yaser Abu-Lebdeh

11 July 2025 in ECS Meeting Abstracts
Verified
Journal Article
Closed access
HKHafsah Azfar Khan
Hafsah Azfar Khan
ZKZouina Karkar
Zouina Karkar
EBElena A. Baranova
Elena A. Baranova
YAYaser A. Abu-Lebdeh
Yaser A. Abu-Lebdeh
High voltage (4.7V) spinel LiMn1.5Ni0.5O4 (LMNO) is a promising cathode material for next generation lithium batteries with high energy densities. Moreover, the usage of Li1.3Al0.3Ti1.7(PO4) (LATP)-coated LMNO enables better cycling performance and higher rate capability [1]. The energy density of the Li-ion batteries can be further improved by increasing cathode thickness, as illustrated in Fig. 1. Hence, when combined with high-voltage cathode materials, thick electrodes are expected to deliver higher energy density, improved capacity, and longer battery life. However, thick electrodes often exhibit lower rate capabilities due to higher charge transfer resistance and high tortuosity. Additionally, there are physical limitations while preparing electrodes using the solvent-casting method beyond a certain thickness due to the occurrence of cracking and delamination during the drying process; this experimentally determined thickness range is highlighted in Fig. 1. Moreover, as electrode thickness increases, there is a greater risk of inadequate Li-ion transport. Ultimately, several parameters including the ratio of solids in the cathode slurry, cathode porosity, and cathode mass loading affect the electrochemical performance of the cathode. In this study, cathode slurries were prepared, and their rheological properties were determined at 25 oC. Cathodes were prepared through the conventional solvent-casting method at various thicknesses and solid ratios to determine the ideal slurry solid ratio, thickness, and porosity to achieve exceptional electrochemical performance. We found that increasing cathode thickness improved specific discharge capacity up to a certain point, after which the capacity began to diminish once again. The optimal thickness and solid ratio were 70 μm and 42.5%, respectively, at which the highest specific discharge capacity of 147 mAh g-1 was achieved at a C-rate of 0.05 C with capacity retention of 85% after 100 cycles. At thicknesses higher than 100 μm, the specific discharge capacity was about 120 mAh g-1 at 0.05 C which may be due to higher ion transport resistance in thicker cathodes and high tortuosity within the cathode microstructure. Figure 1