Ali A. Ati

Ali A. Ati

Auto-generated profile, based on publicly available information

Ali A. Ati

Oil & Gas Engineering College, University of Technology, Baghdad, Iraq

Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
18 January 2021 in Journal of Materials Science: Materials in Electronics
Verified
Journal Article
Closed access
PDF file
AAAli A. Ati
Ali A. Ati
AAAlyaa H. Abdalsalam
Alyaa H. Abdalsalam
AHAli S. Hasan
Ali S. Hasan

16 March 2023 in Polymer Bulletin
Verified
Journal Article
Closed access
PDF file
SMSaja Mohsen
Saja Mohsen
AAAlyaa H. Alsabih
Alyaa H. Alsabih
AAAli A. Ati
Ali A. Ati
MAMakarim H. Abdulkareem
Makarim H. Abdulkareem
ARAhmed A. Ramadhan
Ahmed A. Ramadhan
ZAZeena Yassen Abbas
Zeena Yassen Abbas

3 February 2025 in Journal of Materials Science: Materials in Electronics
Verified
Journal Article
Closed access
PDF file
AAAli A. Ati
Ali A. Ati
AAAlyaa H. Abdalsalam
Alyaa H. Abdalsalam
SASaja Mohsin Alardhi
Saja Mohsin Alardhi
SDS. Dabagh
S. Dabagh
ASA. A. Salim
A. A. Salim
MTMalaa M. Taki
Malaa M. Taki

4 March 2016 in Materials Science Forum
Verified
Journal Article
Closed access
PDF file
RRRizuan Mohd Rosnan
Rizuan Mohd Rosnan
ZOZulkafli Othaman
Zulkafli Othaman
AAAli A. Ati
Ali A. Ati
RHRosli Hussin
Rosli Hussin
SDShadab Dabagh
Shadab Dabagh
SZSamad Zare
Samad Zare
This study evaluates the structural and magnetic properties of Ni-Mg substituted Cobalt ferrite samples prepared through the co-precipitation method. The nominal compositions Co0.5Ni0.5−xMgx Fe2O4 in the range x = 0.1 have been synthesized and then was sintered at temperature at 700 and 1000°C in the furnace for 10 hour with a heating rate of 5°C/min. The prepared nanoferrites were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM) and vibration sample magnetometer (VSM). XRD confirmed formation of single phase spinel ferrite with average crystalline size in the range of 27–33 nm. The lattice constant (a), cell volume (V) and X-ray density (ρx) are also calculated from XRD data. Lattice constant (a) decreases with an increase of sintering temperature. Further information about the structure and morphology of the nanoferrites was obtained from FESEM and results are in good agreement with XRD. Saturation magnetization showed increasing trend with sintering temperature from 700 to 1000°C.

5 July 2022 in Research Square
Verified
Preprint
Open access
PDF file
SASaja M. Alardhi
Saja M. Alardhi
AAAlyaa H. Abdalsalm
Alyaa H. Abdalsalm
AAAli A. Ati
Ali A. Ati
MAMakarim H. Abdulkareem
Makarim H. Abdulkareem
ARAhmed A. Ramadhan
Ahmed A. Ramadhan
ZAZeena Yassen Abbas
Zeena Yassen Abbas
Polyaniline PANi/zinc oxide ZnO nanocomposite has been chemically synthesized by using formic acid. ZnO/PANi nanocomposites containing different weight content of ZnO nanoparticles (10, 20, and 30 wt%). ZnO nanoparticles were prepared by co-precipitation method. Characteristics such as structural, morphological and absorption of the prepared nanocomposites were studied by XRD, FTIR, SEM and UV–vis spectra. X-ray diffraction of zinc oxide nanoparticles confirmed formation of hexagonal wurtzite crystalline structure, also the substituted zinc oxide nanoparticles in different percentage to semi-crystalline polyaniline indicating nearly the same crystalline structure of ZnO/PANi nanocomposites. The Fourier Transform Infrared Spectra (FT-IR) of ZnO nanoparticles, PANi and their composites have been analyzed in the frequency range between 400–4000 cm− 1. The characteristic FT-IR peaks of ZnO nanoparticles show shifts to lower wave numbers in all composites. These observed effects may be due to conjugation and some chemical interactions between ZnO nanoparticles and PANI molecular chain. The results confirmed that the PANI successfully grown on surface of ZnO nanoparticles. The ZnO nanoparticles, PANI and ZnO/PANi nanocomposites were further applied to remove methylene orange dye, the effect of pH, initial dye concertation and ZnO nanoparticles dose were investigated via a batch experimental. According to the results, that the hybrid composite of ZnO/PANi increased the photo degradation of methylene orange dye molecules in aqueous solution compared with parent materials. Maximum removal efficiencies at optimum conditions were higher than 97% at pH 11, concentration of dye:10 mg/l, time equal 40 min and dose 0.1 g of PANi/ZnO.

7 July 2022 in Research Square
Verified
Preprint
Open access
PDF file
SASaja M. Alardhi
Saja M. Alardhi
AAAlyaa H. Abdalsalm
Alyaa H. Abdalsalm
AAAli A. Ati
Ali A. Ati
MAMakarim H. Abdulkareem
Makarim H. Abdulkareem
ARAhmed A. Ramadhan
Ahmed A. Ramadhan
ZAZeena Yassen Abbas
Zeena Yassen Abbas
Polyaniline PANi/zinc oxide ZnO nanocomposite has been chemically synthesized by using formic acid. ZnO/PANi nanocomposites containing different weight content of ZnO nanoparticles (10, 20, and 30 wt%). ZnO nanoparticles were prepared by co-precipitation method. Characteristics such as structural, morphological and absorption of the prepared nanocomposites were studied by XRD, FTIR, SEM and UV–vis spectra. X-ray diffraction of zinc oxide nanoparticles confirmed formation of hexagonal wurtzite crystalline structure, also the substituted zinc oxide nanoparticles in different percentage to semi-crystalline polyaniline indicating nearly the same crystalline structure of ZnO/PANi nanocomposites. The Fourier Transform Infrared Spectra (FT-IR) of ZnO nanoparticles, PANi and their composites have been analyzed in the frequency range between 400–4000 cm− 1. The characteristic FT-IR peaks of ZnO nanoparticles show shifts to lower wave numbers in all composites. These observed effects may be due to conjugation and some chemical interactions between ZnO nanoparticles and PANI molecular chain. The results confirmed that the PANI successfully grown on surface of ZnO nanoparticles. The ZnO nanoparticles, PANI and ZnO/PANi nanocomposites were further applied to remove methylene orange dye, the effect of pH, initial dye concertation and ZnO nanoparticles dose were investigated via a batch experimental. According to the results, that the hybrid composite of ZnO/PANi increased the photo degradation of methylene orange dye molecules in aqueous solution compared with parent materials. Maximum removal efficiencies at optimum conditions were higher than 97% at pH 11, concentration of dye:10 mg/l, time equal 40 min and dose 0.1 g of PANi/ZnO.