Friction spot welding (FSpW) is a solid state welding process suitable for producing spot-like joints, especially in lightweight materials, which are particularly interesting due to the weight saving potential. The plunging of an especially designed non-consumable and rotating tool creates a connection between overlapped sheets through frictional heat and plastic deformation. Minimum material loss is observed, and therefore a fully consolidated joint with flat surface (no keyhole) is obtained. In the current study, the effect of FSpW parameters, such as rotational speed, plunge depth and dwell time, on lap shear strength of AZ31 magnesium alloy joints was investigated. The optimization of input process parameters was carried out through Taguchi approach of DOE. Analysis of variance was applied to determine the individual importance of each parameter. Main effect plots were used to indicate the best levels for maximizing lap shear strength. The results show that tool plunge depth has the higher effect on the weld strength, followed by rotational speed and dwell time.
Friction surfacing (FS) is an advanced solid state process in surface modification with increasing applications in reclaiming worn parts, hardfacing and corrosion protection. The advantages of the process are that materials are deposited in the solid state and the resultant forged microstructure which leads to enhanced mechanical properties. As no melting takes place, the process allows joining of dissimilar materials while avoiding several fusion related problems. The present study addresses the deposition of AA5083-H112 coatings over AA2024-T3 substrates focusing on the influence of the main process parameters such as axial force, rotational speed and deposition speed, in the mechanical properties of the deposits. A performance and geometric analysis of the depositions are also presented. Sound aluminum coatings were produced; plastic deformation and heat generation promotes a dynamic recrystallization of the anisotropic consumable rod, resulting in a fine and homogeneous deposit. The coating presented an increase in ultimate tensile strength and failure deformation of 9% and 6%, respectively. Deposition efficiency between 25 and 50% were obtained, with a maximum of 48% average efficiency observed with 800 RPM, 12 kN and 16 mm/s.
The influence of the weld metal chemistry on the stress corrosion cracking (SCC) susceptibility of dissimilar weldments between 310S austenitic stainless steel and 2304 duplex steels was investigated by constant load tests and microstructural examination. Two filler metals (E309L and E2209) were used to produce fusion zones of different chemical compositions. The SCC results showed that the heat affected zone (HAZ) on the 2304 base metal side of the weldments was the most susceptible region to SCC for both filler metals tested. The SCC results also showed that the weldments with 2209 duplex steel filler metal presented the best SCC resistance when compared to the weldments with E309L filler metal. The lower SCC resistance of the dissimilar joint with 309L austenitic steel filler metal may be attributed to (1) the presence of brittle chi/sigma phase in the HAZ on the 2304 base metal, which produced SC cracks in this region and (2) the presence of a semi-continuous delta-ferrite network in the fusion zone which favored the nucleation and propagation of SC cracks from the fusion zone to HAZ of the 2304 stainless steel. Thus, the SC cracks from the fusion zone associated with the SC cracks of 2304 HAZ decreased considerably the time-of-fracture on this region, where the fracture occurred. Although the dissimilar weldment with E2209 filler metal also presented SC cracks in the HAZ on the 2304 side, it did not present the delta ferrite network in the fusion zone due to its chemical composition. Fractography analyses showed that the mixed fracture mode was predominant for both filler metals used.