Steel fiber embedded in concrete serves to reduce crack development and prevent crack growth at the macroscopic level of the concrete matrix. Steel fiber-reinforced concrete (SFRC) with high compressive concrete strength is affected primarily by the dimensions, shape, content, aspect ratio, and tensile strength of the embedded steel fiber. In this study, double-ended hook steel fiber was used in SFRC with a concrete compressive strength of 80 MPa. This fiber was used for the study variables with two aspect ratios (64, 80) and tensile strength values up to 1600 MPa. The flexural performance of the SFRC specimens was evaluated using crack mouth open displacement tests, and the test results were compared with code provisions. A modified reinforcement index was also used to quantify the flexural performance based on comparisons with fracture energy.
In order to assess the bond behavior of deformed steel rebars in recycled-aggregate concrete (RAC) incorporating both fine and coarse recycled aggregate, pull-out tests were carried out in this study on 16-mm diameter deformed steel rebars embedded concentrically in RAC. The concrete was designed using equivalently mixed proportions of both recycled coarse aggregate and recycled fine aggregate. The tests employed five types of recycled aggregate replacement combinations and three types of rebar placement orientation (i.e., vertical bars and two-tiered and three-tiered horizontal bars). Based on the pull-out test results, the maximum bond strength tended to decrease and the slip at the maximum bond strength increased as the average water absorption of the aggregate increased, irrespective of the rebar orientation or placement location within the concrete member. The pull-out test results for the horizontal steel rebars embedded in RAC indicate that the casting position effect could be determined from the mid-depth of the concrete member, irrespective of the member’s height. The normalized bond versus slip relationship between the deformed rebar and the RAC could be predicted using an empirical model based on regression analysis of the experimental data.
This paper presents an investigation of the characterization of cement mortar containing phase change materials (PCMs) in order to control the development of hydration heat. The study examined microstructural characteristics and properties of cement mortar with PCMs such as flow, compressive strength, and flexural strength. This research involved two types of PCM and up to 15% cement added to cement mortar mixtures. The two types of PCM used in this study are PCM with barium (PCM-Ba) and PCM with strontium (PCM-Sr). The experimental results indicate that both the incremental temperature rise and the maximum temperature release time of PCM up to 5% addition are delayed. Both PCM-Ba and PCM-Sr are effective in reducing the development of hydration heat. The microstructural analysis results show that the crystalloid content of cement mortar without PCMs is about 3% more from cement mortar with PCMs, regardless of the type of PCMs used, and that no significant difference is evident in the formation of crystals between cement mortar with and without PCMs.
This study investigated the effects of shrinkage compensation on the tensile and cracking responses of strain-hardening cement composite (SHCC) by adding calcium sulfoaluminate (CSA)-based expansive additive (EXA) to the mixture. Such responses are closely related to the durability of concrete structures, of dumbbell-shaped SHCC specimens, and reinforced SHCC ties. For this study, two SHCC mixtures and a conventional concrete mixture with a specific compressive strength value of 30 MPa were prepared and measured in terms of shrinkage history, compressive strength, flexural strength, and direct tensile strength. The test results show that the mechanical properties of shrinkage-compensated SHCC with 10% CSA-based EXA are superior to those of conventional SHCC and concrete mixtures. Also, reinforced tension ties with shrinkage-compensated SHCC exhibited the best multiple cracking and tension-stiffening behavior among the three types of tension ties tested. The results show that shrinkage compensation using CSA-based EXA in SHCC with rich mixture is effective for resisting crack damage. Shrinkage-compensated SHCC may be used for civil infrastructure facilities that require high levels of durability and are exposed to extreme environments.