W. Solano-Alvarez

W. Solano-Alvarez

Auto-generated profile, based on publicly available information

W. Solano-Alvarez

Department of Materials Science and Metallurgy, University of Cambridge, UK

Research Focus & Metrics

Academic Career Length

13Years (2014-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
11 July 2014 in Metallurgical and Materials Transactions A
Verified
Journal Article
Closed access
PDF file
WSW. Solano-Alvarez
W. Solano-Alvarez
HBH. K. D. H. Bhadeshia
H. K. D. H. Bhadeshia

1 July 2015 in Materials Science and Technology
Verified
Journal Article
Open access
HBH. K. D. H. Bhadeshia
H. K. D. H. Bhadeshia
WSW. Solano-Alvarez
W. Solano-Alvarez
One form of damage due to rolling contact fatigue is the formation of localised regions of extremely hard material forming within the body of a bearing. These regions have a relatively homogeneous structure and hence etch mildly with respect to the surrounding unaffected matrix. They, therefore, appear white in a darker background when examined using optical microscopy. We assess here the cause of this damage and propose solutions that are backed by evidence that already is available. The issue is important because of the spate of unexpected failures in large wind turbine bearings and of generic importance in determining the life of more well behaved bearing applications.

1 November 2014 in Materials Science and Engineering: A
Verified
Journal Article
Closed access
WSW. Solano-Alvarez
W. Solano-Alvarez
Ed PickeringEd Pickering
Ed Pickering
HBH.K.D.H. Bhadeshia
H.K.D.H. Bhadeshia

1 December 2016 in Acta Materialia
Verified
Journal Article
Open access
WSW. Solano-Alvarez
W. Solano-Alvarez
Ed PickeringEd Pickering
Ed Pickering
MPM.J. Peet
M.J. Peet
KMK.L. Moore
K.L. Moore
JJJ. Jaiswal
J. Jaiswal
HBH.K.D.H. Bhadeshia
H.K.D.H. Bhadeshia
© 2016 Acta Materialia Inc.There has been a great deal of work on the formation of hard white-etching regions in conventional bearing steels such as 1C-1.5Cr wt% when subjected repeatedly to rolling contact stresses. The regions are a consequence of localised mechanical attrition across microcrack faces and mixing, which refine the local structure and force cementite to dissolve. This white-etching matter is often associated with brittle phenomena because the hardness can exceed 1100 HV. In contrast, carbide-free mixtures of bainitic ferrite and retained austenite when subjected to the same loading have been unexpectedly found not to develop the characteristic patches of hard material and to show instead signs of ductility in the attrited regions. The work presented here shows that the white-etching areas that develop in carbide-free bainite are softer than their surroundings, whether they are in hard nanostructured bainite destined for bearing applications or when the steel is designed for the manufacture of rails. Advanced characterisation tools were used for the first time to understand carbon redistribution during its formation. The deep interest about soft white-etching matter originates from the idea that it could lead to the reduction in premature failure of wind turbine gearbox bearings and white-etching layer grinding of rails.This is the final version of the article. It first appeared from Elsevier via http://dx.doi.org/10.1016/j.actamat.2016.09.01

1 November 2017 in Materials Science and Engineering: A
Verified
Journal Article
Open access
WSW. Solano-Alvarez
W. Solano-Alvarez
MPM.J. Peet
M.J. Peet
Ed PickeringEd Pickering
Ed Pickering
JJJ. Jaiswal
J. Jaiswal
ABAdam Bevan
Adam Bevan
HBH.K.D.H. Bhadeshia
H.K.D.H. Bhadeshia

8 July 2014 in Metallurgical and Materials Transactions A
Verified
Journal Article
Closed access
PDF file
WSW. Solano-Alvarez
W. Solano-Alvarez
HBH. K. D. H. Bhadeshia
H. K. D. H. Bhadeshia