Izumi Muto

Izumi Muto

Auto-generated profile, based on publicly available information

Izumi Muto

Tohoku University

Research Focus & Metrics

Academic Career Length

39Years (1988-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
25 July 2013 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
ACAya Chiba
Aya Chiba
IMIzumi Muto
Izumi Muto
YSYu Sugawara
Yu Sugawara
NHNobuyoshi Hara
Nobuyoshi Hara
Microscopic polarization, scanning transmission electron microscopy, and Raman spectroscopy were performed to ascertain the pit initiation mechanism at MnS inclusions in stainless steels. While the inclusion surfaces dissolved under anodic polarization in 0.1 M Na2SO4 as well as 0.1 and 3 M NaCl solutions, the boundaries between the inclusions and the steel matrix dissolved selectively only in the NaCl solutions. This selective dissolution resulted in the formation of trenches, in which metastable and stable pits were initiated. The trenches were shown to be formed by the active dissolution of the steel sides of the boundaries, where no anomalous phase and no compositionally altered zone was observed. It was found that elemental sulfur was deposited on the inclusions and at the boundaries after anodic polarization in 3 M NaCl. The active dissolution of the steel matrix occurred in solutions in which chloride ions and elemental sulfur coexist. The synergistic effect of the elemental sulfur produced by MnS inclusion and chloride ions is likely to cause the trenches, and the decrease in both pH and potential inside the trenches results in pit initiation.

1 January 2007 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
IMIzumi Muto
Izumi Muto
YIYuta Izumiyama
Yuta Izumiyama
NHNobuyoshi Hara
Nobuyoshi Hara
The electrochemical dissolution of MnS inclusions and pit initiation processes on type 303 stainless steel were investigated by an electrochemical microcell technique. In <mml:math display="inline"><mml:mrow><mml:mn>1</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi mathvariant="normal">M</mml:mi></mml:mrow></mml:math>1M <mml:math display="inline"><mml:mrow><mml:msub><mml:mi mathvariant="normal">Na</mml:mi><mml:mrow><mml:mn>2</mml:mn></mml:mrow></mml:msub><mml:mi mathvariant="normal">S</mml:mi><mml:msub><mml:mi mathvariant="normal">O</mml:mi><mml:mrow><mml:mn>4</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math>Na2SO4 , the electrochemical dissolution of MnS inclusions started at <mml:math display="inline"><mml:mrow><mml:mn>0.1</mml:mn><mml:mo>–</mml:mo><mml:mn>0.3</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi mathvariant="normal">V</mml:mi></mml:mrow></mml:math>0.1–0.3V vs <mml:math display="inline"><mml:mrow><mml:mi mathvariant="normal">Ag</mml:mi><mml:mo>∕</mml:mo><mml:mi mathvariant="normal">Ag</mml:mi><mml:mi mathvariant="normal">Cl</mml:mi><mml:mrow><mml:mo>(</mml:mo><mml:mn>3.33</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi mathvariant="normal">M</mml:mi><mml:mspace width="0.3em"></mml:mspace><mml:mi mathvariant="normal">K</mml:mi><mml:mi mathvariant="normal">Cl</mml:mi><mml:mo>)</mml:mo></mml:mrow></mml:mrow></mml:math>Ag∕AgCl(3.33MKCl) , which was followed by the initiation of a hemispherical and smooth wall pit at MnS/matrix boundary. It was suggested that the dissolution products of MnS inclusions induced the formation of a salt film, which caused localized electropolishing. In <mml:math display="inline"><mml:mrow><mml:mn>0.1</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi mathvariant="normal">M</mml:mi></mml:mrow></mml:math>0.1M NaCl, the onset potential of electrochemical dissolution of MnS inclusions was <mml:math display="inline"><mml:mrow><mml:mn>0.3</mml:mn><mml:mo>–</mml:mo><mml:mn>0.4</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi mathvariant="normal">V</mml:mi></mml:mrow></mml:math>0.3–0.4V and the stable pit growth occurred at a potential of around <mml:math display="inline"><mml:mrow><mml:mn>0.5</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi mathvariant="normal">V</mml:mi></mml:mrow></mml:math>0.5V . Field-emission scanning electron microscopy observations revealed that many metastable pits with a diameter of approximately <mml:math display="inline"><mml:mrow><mml:mn>1</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi>μ</mml:mi><mml:mi mathvariant="normal">m</mml:mi></mml:mrow></mml:math>1μm were formed at MnS/matrix boundary on the specimen, of which the polarization measurement was stopped immediately after stable pit initiation. From a morphological point of view, the metastable pits were found to be very similar to flat-walled etch pits. The dissolution products of MnS inclusions and chloride ions would attack the metal surface newly exposed by dissolution of the inclusions. It is proposed that the chemistry of dissolved species from MnS inclusions have a substantial influence on pit initiation at MnS inclusions.

1 January 2012 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
ACAya Chiba
Aya Chiba
IMIzumi Muto
Izumi Muto
YSYu Sugawara
Yu Sugawara
NHNobuyoshi Hara
Nobuyoshi Hara
A microelectrochemical system for in situ high-resolution optical microscopy was fabricated and applied to the real-time observation of pit initiation at MnS inclusion in type 304 stainless steel in NaCl solutions. It was directly observed that the metastable and stable pits were initiated at the MnS/steel boundaries, and that deep trenches were generated at these boundaries during anodic polarization. The initial rounded form of metastable and stable pits became polygonal in shape within 1 s. After that, the dissolution proceeded in the depth direction with no change in the appearance of the pit as observed externally. In the case of the metastable pitting, the duration of this stage was ca. 1.5 s, and then the pit repassivated, and the polygonal metastable pit remained on the electrode surface. The in-depth growth stage for stable pitting was relatively longer (ca. 3.5 s), and the pit grew deeply into the steel matrix and wrapped beneath the inclusion, leading to the formation of a large occluded cavity, in which the corrosivity considerably exceeded the critical conditions for autocatalytic pit growth. Chloride ions were shown to increase the probability of metastable pit initiation and affected the surface and cross-sectional morphology of stable pits.

1 May 2016 in Corrosion Science
Verified
Journal Article
Open access
MNMasashi Nishimoto
Masashi Nishimoto
JOJunichiro Ogawa
Junichiro Ogawa
IMIzumi Muto
Izumi Muto
YSYu Sugawara
Yu Sugawara
NHNobuyoshi Hara
Nobuyoshi Hara
A sensing plate for the simultaneous measurements of pH and Cl− concentration was fabricated. Terbium–dipicolinic acid complex (Tb–DPA) and quinine sulphate were used to measure the pH and Cl− concentration, respectively. In the incubation period of the crevice corrosion, the pH inside the crevice gradually decreased from 3.0 to ca. 2.0, and the Cl− concentration increases from 0.01 to ca. 0.18M. The generation of the micro-pit led to a sharp decrease in pH to below 0.5 and an increase in the Cl− concentration to above 4M. This situation allowed the crevice corrosion to proceed without spontaneously stopping

1 January 2009 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
IMIzumi Muto
Izumi Muto
DIDaiki Ito
Daiki Ito
NHNobuyoshi Hara
Nobuyoshi Hara

1 October 2012 in Intermetallics
Verified
Journal Article
Closed access
ZDZhenhua Dan
Zhenhua Dan
FQFengxiang Qin
Fengxiang Qin
YSYu Sugawara
Yu Sugawara
IMIzumi Muto
Izumi Muto
NHNobuyoshi Hara
Nobuyoshi Hara