This study aims to develop thermoplastic (TP) and thermoset (TS) based mixed matrix composite using design dependent physical compatibility. Using thermoplastic-based (PLA) skeletal lattices with diverse patterns (gyroid and grid) and different infill densities (10% and 20%) followed by infiltration of two different thermoset resin systems (epoxy and polyurethane-based) using a customized FDM 3D printer equipped with a resin dispensing unit, the optimised design and TP-TS material combination was established for best mechanical performance. Under uniaxial tensile stress, the failure modes of TP gyroid structures with polyurethane-based composites included ‘fiber pull-out’, interfacial debonding and fiber breakage, while epoxy based mixed matrix composites with all design variants demonstrated brittle failure. Higher elongation (higher area under curve) was observed in 20% infilled gyroid patterned composite with polyurethane matrix indicating the capability of operation in mechanical shock absorption application. Electron microscopy-based fractography analysis revealed that thermoset matrix properties governed the fracture modes for the thermoplastic phase. This work focused on the strategic optimisation of both toughness and stiffness of mixed matrix composite components for rapid fabrication of construction materials.
Polymer‐coated ceramic powders (PCCPs) prepared via a thermally induced phase separation (TIPS) process have emerged as a promising alternative for enhancing the processability and mechanical properties of highly filled ceramic polymer compounds. This study investigates the performance of PCCP, specifically alumina particles coated with polybutylene terephthalate (PBT), compared to conventional admix compounds prepared through melt‐mixing. The research explores the viscosity, flowability, packing efficiency, and thermal stability of PCCP at 50 and 60 vol.% solids loadings. The results indicate that PCCP exhibits significantly lower viscosity across all shear rates, with a 54.1% reduction at 1000 s ‒1 compared to admixes at 50% loading, which can help to improve mold filling behavior and reduce processing defects. Additionally, PCCPs demonstrate enhanced powder flowability, as evidenced by a lower Hausner ratio (1.15 for 50% PCCP vs. 1.56 for alumina particles) and high pycnometer density (2.81 g/cm 3 ), suggesting good packing efficiency. At 60% loading, all compounds exhibited significantly increased viscosity, indicating the challenges associated with high solids loading, while PCCP maintained improved rheological performance under these conditions. The findings highlight PCCPs as a better alternative to conventional, ad‐mixed ceramic‒polymer compounds, offering enhanced flow characteristics at industrially relevant shear rates, better packing, and improved thermal behavior, making it a viable option for high‐performance ceramic injection molding applications.