The additive manufacturing of low elastic modulus alloys that have a certain level of porosity for biomedical needs is a growing area of research. Here, we show the results of manufacturing of porous and dense samples by a laser powder bed fusion (LPBF) of Ti-Nb alloy, using two distinctive fusion strategies. The nanostructured Ti-Nb alloy powders were produced by mechanical alloying and have a nanostructured state with nanosized grains up to 90 nm. The manufactured porous samples have pronounced open porosity and advanced roughness, contrary to dense samples with a relatively smooth surface profile. The structure of both types of samples after LPBF is formed by uniaxial grains having micro- and nanosized features. The inner structure of the porous samples is comprised of an open interconnected system of pores. The volume fraction of isolated porosity is 2 vol. % and the total porosity is 20 vol. %. Cell viability was assessed in vitro for 3 and 7 days using the MG63 cell line. With longer culture periods, cells showed an increased cell density over the entire surface of a porous Ti-Nb sample. Both types of samples are not cytotoxic and could be used for further in vivo studies.
Mathematical relation between roughness of the surface layer of the sintered article and layer-by-layer laser sintering modes obtained from experiments conducted using copper powder material PMS-1. Authors suggest that split manufacturing process of an article and its inner part must be split to roughing, semi-finishing and finishing modes.
1 August 2016 in IOP Conference Series: Materials Science and Engineering
Various process variables influence on the quality of the end product when SLM (Selective Laser Melting) synthesizing items of powder materials. The authors of the paper suggest using the model of distributing the temperature fields when forming single tracks and layers of copper powder PMS-1. Relying on the results of modeling it is proposed to reduce melting of powder particles out of the scanning area.
The influence of technological modes of sintering: the displacement velocity of laser beam V, laser power P, scanning step S and preheating temperature of powder material t on the quality of sintered surface layer of aluminum powder PA-4, copper powder PMS-1 and cobalt- chromium-molybdenum powder DSK-F75 were studied.
The paper presents results of research on a method of determining a geometric condition of a sintered surface using an instrumental digital microscope. The results of experimental studies of effects of laser irradiation technological modes on roughness of the cobalt chrome molybdenum powder DSK-F75 sintered layer are presented. Differentiation of modes of product surface and its internal volume formation into rough, semi-finishing and finishing are proposed.