The recent progress and development of corundum-structured III-oxide semiconductors are reviewed. They allow bandgap engineering from 3.7 to ∼9 eV and function engineering, leading to highly durable electronic devices and deep ultraviolet optical devices as well as multifunctional devices. Mist chemical vapor deposition can be a simple and safe growth technology and is advantageous for reducing energy and cost for the growth. This is favorable for the wide commercial use of devices at low cost. The III-oxide semiconductors are promising candidates for new devices contributing to sustainable social, economic, and technological development for the future.
31 October 2016 in Japanese Journal of Applied Physics
Homoepitaxial single-crystal beta gallium oxide (β-Ga2O3) films were fabricated by the mist chemical vapor deposition method. The crystallinity of the films grown markedly depended on growth temperature, and the optimum growth temperatures were found to be 700–800 °C. Using unintentionally doped β-Ga2O3 films grown on Sn-doped β-Ga2O3(010) substrates, the fabrication of Schottky barrier diodes was demonstrated. Furthermore, we fabricated electrically conductive Sn-doped β-Ga2O3 films on semi-insulating Fe-doped β-Ga2O3(010) substrates. The carrier concentrations were between 1 × 1018 and 5 × 1020 cm−3. The Hall mobility was 45 cm2 V−1 s−1 at the carrier concentration of 1 × 1018 cm−3.
Efforts have been made to reduce the density of defects in corundum-structured α-Ga2O3 thin films on sapphire substrates by applying quasi-graded α-(AlxGa1−x)2O3 buffer layers. Transmission electron microscopy images revealed that most strains were located in the α-(AlxGa1−x)2O3 buffer layers, and that the total density of dislocations in the α-Ga2O3 thin films was successfully decreased by more than one order of magnitude compared with that without buffer layers, that is, the screw and edge dislocation densities were about 3 × 108 and 6 × 108 cm−2, respectively.
Ultra-wide bandgap p-type α-(Ir,Ga)2O3 films with bandgaps of up to 4.3 eV have been obtained by unintentional doping or Mg doping. For Mg-doped films, Hall-effect measurements revealed a hole concentration of 9.9 × 1018 to 8.1 × 1019 cm−3 and a mobility of 0.13 − 0.92 cm2/V s, respectively. A preliminary test of a pn junction diode composed of p-type α-(Ir,Ga)2O3 and n-type α-Ga2O3 did not show catastrophic breakdown in the reverse direction until 100 V and the current on/off ratio at +3 V/−3V was 5 × 105. Since α-(Ir,Ga)2O3 and α-Ga2O3 take the same crystal structure and are well lattice-matched (with a lattice mismatch of <0.3%), the formation of a high-quality pn heterojunction is encouraged; this is one of the advantages of the corundum material system.