15 March 2018 in Journal of the Electrochemical Society
Carbon corrosion is an important degradation mechanism that can impair PEMFC performance through the destruction of catalyst connectivity, collapse of the electrode pore structure, loss of hydrophobic character, and an increase of the catalyst particle size. In this study, carbon corrosion was quantified in situ by measurement of carbon dioxide in the fuel cell exhaust gases through non-dispersive infrared spectroscopy during simulated drive cycle operations consisting of potential cycling with varying upper and lower potential limits. These studies were conducted for three different types of carbon supports. A reduction in the catalyst layer thickness was observed during a simulated drive cycle operation with a concomitant decrease in catalyst layer porosity, which led to performance losses due to increased mass transport limitations. The observed thickness reduction was primarily due to compaction of the catalyst layer, with the actual mass of carbon oxidation (loss) contributing only a small fraction (< 20%). The dynamics of carbon corrosion are presented along with a model that simulates the transient and dynamic corrosion rates observed in our experiments. Accelerated carbon corrosion stress tests are presented and their effects are compared to those observed for the drive cycle test.
15 May 2018 in Journal of the Electrochemical Society
The U.S. Department of Energy (DOE) set the 2020 durability target for polymer electrolyte membrane fuel cell transportation applications at 5000 hours. Since it is impractical to test every fuel cell for this length of time, there is ever increasing interest in developing accelerated stress tests (ASTs) that can accurately simulate the material component degradation in the membrane electrode assembly (MEA) observed under automotive operating conditions, but over a much shorter time frame. In this work, a square-wave catalyst AST was examined that shows a 5X time acceleration factor over the triangle-wave catalyst AST and a 25X time acceleration factor over the modified wet drive-cycle catalyst durability protocol, significantly decreasing the testing time. These acceleration factors were correlated to the platinum (Pt) particle size increase and associated decrease in electrochemical surface area (ECSA). This square-wave AST has been adopted by the DOE as a standard protocol to evaluate catalyst durability. We also compare three catalyst-durability protocols using state-of-the-art platinum-cobalt catalysts supported on high surface area carbon (SOA Pt-Co/HSAC) in the cathode catalyst layer. The results for each of the three tests showed both catalyst particle size increase and transition metal leaching. Moreover the acceleration factors for the alloy catalysts were smaller due to Co leaching being the predominant mechanism of voltage decay in ∼5 nm PtCo/C catalysts. Finally, an extremely harsh carbon corrosion AST was run using the same SOA Pt-Co/HSAC catalyst. This showed minimal change in particle size and a low percentage Co loss from the cathode catalyst particles, despite a significant loss in catalyst layer thickness and cell performance. The carbon corrosion rates during these various ASTs were directly measured by monitoring the CO2 emission from the cathode, further confirming the ability of the square-wave AST to evaluate the electro-catalyst independently of the support.
8 November 2014 in Journal of the Electrochemical Society
AAAlireza Sadeghi Alavijeh
+2
Regular durability testing of heavy duty fuel cell systems for transit bus application requires several thousand hours of operation, which is costly and time consuming. Alternatively, accelerated durability tests are able to generate failure modes observed in field operation in a compressed time period, by applying enhanced levels of stress. The objective of the present work is to design and validate an accelerated membrane durability test (AMDT) for heavy duty fuel cells under bus related conditions. The proposed AMDT generates bus relevant membrane failure modes in a few hundred hours, which is more than an order of magnitude faster than for regular duty cycle testing. Elevated voltage, temperature, and oxidant levels are used to accelerate membrane chemical stress, while relative humidity (RH) cycling is used to induce mechanical stress. RH cycling is found to significantly reduce membrane life-time compared to constant RH conditions. The role of a platinum band in the membrane is investigated and membranes with Pt bands demonstrate a considerable life-time extension under AMDT conditions, with minimal membrane degradation. Overall, this research serves to establish a benchmark AMDT that can rapidly and reliably evaluate membrane stability under simulated heavy duty fuel cell conditions.
1 December 2016 in Journal of Power Sources
1 January 2013 in ECS Electrochemistry Letters
Enhancing the durability of fuel cells for the transportation sector requires a better understanding of the fundamental processes that cause degradation. Field-operated PEMFCs have been shown to develop a thin parallel band of Pt inside the membrane. Reports on the effect of the Pt band on membrane durability are contradictory. Here, we examined the influence of the Pt band by performing in situ and ex situ membrane degradation tests. We report that the Pt band significantly decreases the rate of membrane degradation, thereby enhancing its longevity.
22 April 2019 in Journal of the Electrochemical Society
PtCo/C and Pt/C catalyst powders were incorporated into electrospun nanofiber and conventional sprayed cathode membrane-electrode-assemblies (MEAs) at a fixed electrode loading of 0.1 mgPt/cm2. The binder for PtCo/C nanofiber cathodes and Pt/C nanofiber anodes was a mixture of Nafion and poly(acrylic acid) (PAA), whereas the sprayed electrode MEAs utilized a neat Nafion binder. The structure of electrospun fibers was analyzed by scanning transmission electron microscopy (STEM) and energy-dispersive X-ray spectroscopy (EDS), which showed that the fibers were ∼30% porous with a uniform distribution of catalyst and binder in the axial and radial fiber directions. The initial performance of nanofiber MEAs at 80°C was 20% better than the sprayed electrode MEA (a maximum power density of 1,045 mW/cm2 vs. 869 mW/cm2). The benefit of the nanofiber electrode morphology was most evident at end-of-test (after a metal dissolution accelerated stress test), where power densities dropped by only 8%, after 30,000 square wave voltage cycles (0.6 V to 0.95 V), as compared to a 35% drop in the maximum power for the sprayed electrode MEA. The use of a recovery protocol improved the initial performance of a nanofiber MEA by ∼13%, to 1,070 mW/cm2 at 0.65 V, and increased the power after a metal dissolution stress test by 5–10% (e.g. 840 mW/cm2 at 0.65 V after 30,000 voltage cycles). At rated power, the nanofiber MEA generated more than 1,000 mW/cm2 at 99°C and a pressure of 250 kPaabs. The high performance and durability of PtCo/C nanofiber cathode MEAs is due to the combined effects of a highly active cathode catalyst and the unique nanofiber electrode morphology, where there is a uniform distribution of catalyst and binder (no agglomeration) and short transport pathways across the submicron diameter fibers (which lowers gas transfer resistance and facilitates water removal from the cathode).