This review describes the advancements in the field of Ni-rich NCM cathodes in terms of manufacturing processes, material challenges, modification techniques, and future research directions, and discusses the correlation between the synthesis and electrochemical performance.
Production of low-cobalt/cobalt-free cathodes, recycling, continuous manufacturing and fast-charging ability is important. They determine the cell manufacturing cost, supply-chain stability, environmental benignity.
The microparticle quality and reproducibility of Li(Ni0.8Co0.1Mn0.1)O2 (NCM811) cathode materials are important for Li-ion battery performance but can be challenging to control directly from synthesis. Here, a scalable reproducible synthesis process is designed based on slug flow to rapidly generate uniform micron-size spherical-shape NCM oxalate precursor microparticles at 25-34 °C. The whole process takes only 10 min, from solution mixing to precursor microparticle generation, without needing aging that typically takes hours. These oxalate precursors are convertible to spherical-shape NCM811 oxide microparticles, through a preliminary design of low heating rates (e.g., 0.1 and 0.8 °C/min) for calcination and lithiation. The outcome oxide cathode particles also demonstrate improved tap density (e.g., 2.4 g mL-1 for NCM811) and good specific capacity (202 mAh g-1 at 0.1 C) in coin cells and reasonably good cycling performance with LiF coating.
Nanostructured silicon (Si) anodes with various dimensions (0- or 1D) are widely explored in the manufacturing of high-energy-density lithium-ion batteries (LIBs) to mitigate volume expansion during cycling. However, most of them suffer from multiple issues, such as phase impurity, inhomogeneity in particle size, and poor mechanical strength, resulting in poor rate capability, cycle performance, and Coulombic efficiency. In this work, a modified physical vapor deposition technique, known as the glancing angle deposition (GLAD) method, is utilized to produce pure Si nanospring arrays on Cu foil. The nanospring architecture, with controlled dimensions, facilitates Li+ diffusion throughout the amorphous Si and offers good rate performance. In this case, electrochemical polishing of Cu foil has played a pivotal role to achieve a very high specific capacity of 2800 mAh g-1 at 300 mA g-1 and a very good rate capability of up to 4500 mA g-1. The electrochemical polishing facilitates uniform deposition of the Si nanosprings on the Cu surface and offers better structural robustness compared to the unpolished one.
Continuous production of good quality low-cobalt Ni-rich cathode is needed as it can offer high capacity suitable for electric vehicles. However, the low-cobalt NCM-based materials suffer from a high cation mixing and poor rate capability. Also, proper optimization of co-precipitation reaction parameters as well as the manufacturing platform are needed to obtain NCM-precursor particles with uniform particle size and morphology. In order to address all the issues, in this work, a slug-flow-based manufacturing platform is utilized for the continuous production of Fe3+ substituted Ni0.85Co(0.1−x)Mn0.05FexC2O4 (where x = 0, 0.02, 0.04) precursors. The slug-flow manufacturing produces precursor particles with high yield and uniformity. The effect of reactants concentration on the product yield and composition is analyzed through mathematical modelling. Finally, the electrochemical performance of the Ni-rich cathodes with various amounts of Co and Fe content is analyzed through rate capability, cycling stability, and impedance analysis. This work provides key insight into: (i) reactor design for continuous production; (ii) mathematical modelling of the precipitation reaction parameter; and (iii) a detail study of the effect of Co-substitution with Fe3+ in Ni-rich NCM on its physical properties as well as electrochemical performance. We find that an intermediate Fe content provides optimum cathode with desired properties.