1 October 2024 in Nature Materials
The sodium (Na) superionic conductor is a key component that could revolutionize the energy density and safety of conventional Na-ion batteries. However, existing Na superionic conductors are primarily based on a single-anion framework, each presenting inherent advantages and disadvantages. Here we introduce a family of amorphous Na-ion conductors (Na2O2–MCly, M = Hf, Zr and Ta) based on the dual-anion framework of oxychloride. Benefiting from a dual-anion chemistry and with the resulting distinctive structures, Na2O2–MCly electrolytes exhibit room-temperature ionic conductivities up to 2.0 mS cm−1, wide electrochemical stability windows and desirable mechanical properties. All-solid-state Na-ion batteries incorporating amorphous Na2O2–HfCl4 electrolyte and a Na0.85Mn0.5Ni0.4Fe0.1O2 cathode exhibit a superior rate capability and long-term cycle stability, with 78% capacity retention after 700 cycles under 0.2 C (1C = 120 mA g−1) at room temperature. The discoveries in this work could trigger a new wave of enthusiasm for exploring new superionic conductors beyond those based on a single-anion framework.
1 November 2018 in Nano Energy
25 November 2024 in Nature Nanotechnology
The advancement of all-solid-state lithium metal batteries requires breakthroughs in solid-state electrolytes (SSEs) for the suppression of lithium dendrite growth at high current densities and high capacities (>3 mAh cm−2) and innovation of SSEs in terms of crystal structure, ionic conductivity and rigidness. Here we report a superionic conducting, highly lithium-compatible and air-stable vacancy-rich β-Li3N SSE. This vacancy-rich β-Li3N SSE shows a high ionic conductivity of 2.14 × 10−3 S cm−1 at 25 °C and surpasses almost all the reported nitride-based SSEs. A Li- and N-vacancy-mediated fast lithium-ion migration mechanism is unravelled regarding vacancy-triggered reduced activation energy and increased mobile lithium-ion population. All-solid-state lithium symmetric cells using vacancy-rich β-Li3N achieve breakthroughs in high critical current densities up to 45 mA cm−2 and high capacities up to 7.5 mAh cm−2, and ultra-stable lithium stripping and plating processes over 2,000 cycles. The high lithium compatibility mechanism of vacancy-rich β-Li3N is unveiled as intrinsic stability to lithium metal. In addition, β-Li3N possesses excellent air stability through the formation of protection surfaces. All-solid-state lithium metal batteries using the vacancy-rich β-Li3N as SSE interlayers and lithium cobalt oxide (LCO) and Ni-rich LiNi0.83Co0.11Mn0.06O2 (NCM83) cathodes exhibit excellent battery performance. Extremely stable cycling performance is demonstrated with high capacity retentions of 82.05% with 95.2 mAh g−1 over 5,000 cycles at 1.0 C for LCO and 92.5% with 153.6 mAh g−1 over 3,500 cycles at 1.0 C for NCM83. Utilizing the vacancy-rich β-Li3N SSE and NCM83 cathodes, the all-solid-state lithium metal batteries successfully accomplished mild rapid charge and discharge rates up to 5.0 C, retaining 60.47% of the capacity. Notably, these batteries exhibited a high areal capacity, registering approximately 5.0 mAh cm−2 for the compact pellet-type cells and around 2.2 mAh cm−2 for the all-solid-state lithium metal pouch cells.
28 August 2017 in Biotechnology Journal
1 November 2014 in Ceramics International