Hot extrusion forming is one of the best cost-effective processing methods to obtain high-strength aluminum alloys. In order to obtain high performance 2024 aluminum alloy for the aero and automobile industries, this research comprehensively uses heat treatment and reverse isothermal extrusion technology to prepare 2024 alloy. The effects of homogenization, extrusion and post-extrusion annealing treatment on the microstructure and mechanical properties of 2024 aluminum alloy were discussed in detail. The results indicate that the grain refinement of the extruded alloy material is significant. The coarse eutectic microstructure at the grain boundaries was refined, and these grains tended to be uniformly distributed after the annealing treatment. Extruded 2024 aluminum alloy material mainly has S (Al2CuMg) and Al7Cu2Fe second phases. The appearance of a large number of S phases led to a significant improvement in the properties of the alloy with an increase in tensile strength and elongation of 176% and 547%, respectively. In addition, EBSD analysis showed a significant meritocratic growth in the extrusion direction with the appearance of Copper {112} rolling weaving, which led to process hardening and the strength improvement of the alloy.
7 November 2024 in Journal of Materials Research and Technology
A new welding method, flux bands constricting arc (FBCA) welding, is proposed to compensate for the shortage of insufficient weld width of laser welding T-joints in high steel sandwich panels. The arc behavior (arc burning position, arc shape, arc heat, and arc stability) before and after sticking the flux bands (GMAW and FBCA welding) to the ultra-narrow gap groove was tested. Results indicate that flux bands have solid-wall constricting effect (SWCE) and thermo-compression effect (TCE) on the arc and self-producing slag and gas function in FBCA welding. In ultra-narrow gap groove, the arc burning position climbing up phenomenon (APCP) occurs without flux bands. The SWCE of flux bands on the arc effectively suppresses the APCP because of the insulation of flux bands. In the FBCA welding process, the effective heating area of the arc is increased by at least 5 mm2 compared with that in GMAW. When the groove gap decreases, flux bands not only compress the arc from an inverted bell shape to a rectangular shape, but also make the 660 °C isotherm on the core-plate to increase from 3 mm to 8 mm. In the end, the proportion of unstable arc burning time is reduced by 86.85%, the fluctuation of arc voltage and welding current are also significantly reduced by the flux bands because of their SWCE on the arc.