Controlled thermal oxidations of thin copper films at relatively lower temperatures (up to 500°C) leading towards the formation of a single phase of copper oxide are investigated where the oxidation temperature, duration, oxygen partial pressure, film thickness and the crystallographic orientations play very crucial roles to significantly control the final phase of the copper oxide. Thin Cu films of thicknesses 100-1000 nm were deposited on glass and silicon substrates using the vacuum assisted thermal evaporation technique. Oxidations of those Cu films were performed at different temperatures for variable durations in air ambient as well as oxygen ambient conditions. Four probe resistivity measurement, x-ray diffraction (XRD), Raman spectroscopy, ultraviolet–visible (UV-Vis) spectroscopy, scanning electron microscopy (SEM) and x-ray photoemission spectroscopy (XPS) techniques have been used to characterize the oxide films. At a thermodynamic equilibrium, it has been observed that the oxide phase is solely determined by the oxidation temperature, however, the oxygen partial pressure can significantly alter this temperature range. In case of thermal oxidation in air, the initial oxidation of the copper films starts at about 150 °C, but a well ordered crystalline phase of the cuprous oxide (Cu2O) is observed only above 200 °C. However, the cupric oxide (CuO) phase starts to appear only above 320 °C. The details of the oxidation mechanism of the Cu film are explained with a probable schematic model in terms of thermal diffusion as well as the chemical reactivity.
Here, we experimentally and theoretically clarify III-V/Si crystal growth processes. Atomically resolved microscopy shows that monodomain three-dimensional islands are observed at the early stages of AlSb, AlN, and GaP epitaxy on Si, independently of misfit. It is also shown that complete III-V/Si wetting cannot be achieved in most III-V/Si systems. Surface/interface contributions to the free-energy variations are found to be prominent over strain relief processes. We finally propose a general and unified description of III-V/Si growth processes, including a description of the formation of antiphase boundaries.
The electronic band structure and the work function of MgO thin films epitaxially grown on Ag(001) have been investigated using x-ray and ultraviolet photoelectron spectroscopy for various oxide thicknesses. The deposition of thin MgO films on Ag(001) induces a strong diminution in the metal work function. The -type Schottky barrier height is constant at above two MgO monolayers and the experimental value of the ionization potential is . Our results are well consistent with the description of the Schottky barrier height in terms of the Schottky–Mott model corrected by an MgO-induced polarization effect.
Here we clarify the central role of the miscut during group III-V/group IV crystal growth. We show that the miscut impacts the initial antiphase domain distribution, with two distinct nucleation-driven (miscut typically >1°) and terraces-driven (miscut typically <0.1°) regimes. It is then inferred how the antiphase domain distribution mean phase and mean lateral length are affected by the miscut. An experimental confirmation is given through the comparison of antiphase domain distributions in GaP and GaSb/AlSb samples grown on nominal and vicinal Si substrates. The antiphase domain burying step of GaP/Si samples is then observed at the atomic scale by scanning tunneling microscopy. The steps arising from the miscut allow growth rate imbalance between the two phases of the crystal and the growth conditions can deeply modify the imbalance coefficient, as illustrated with GaAs/Si. We finally explain how a monodomain III-V semiconductor configuration can be achieved even on low miscut substrates.
Single-crystalline (001) Fe thin films were prepared by molecular beam epitaxy and covered by epitaxial MgO barriers. The MgO growth was confirmed to be layer by layer as shown by reflection high-energy electron diffraction, which allowed us to prepare Fe films covered by only two atomic planes of MgO for spin polarization measurements. On the one hand, regular x-ray photoemission spectroscopy measurements evidenced a weak hybridization between Fe and O. Moreover, a large Fe magnetic moment at the interface with MgO was shown by x-ray magnetic circular dichroism measurements. These two observations are in agreement with theory. On the other hand, we show that the Fe density of states can be measured by photoemission through the oxide barrier, since the oxide valence band only starts at 4 eV below the Fermi level. Spin-resolved x-ray photoemission measurements performed at ESRF allowed us to demonstrate that the electrons emitted from the (001) Fe layer through the barrier are polarized. A polarization fully integrated in k space and corrected from remanence near 42% was measured.