The authors conducted an in-depth analysis of domestic and foreign literary data, as well as formulated and set the goal of this scientific work. The inoculation of cast Al-based alloy of the AK12 DSTU 2839:1994 with dispersed intermetallic FeCr in the “volume” of the casting mold (CM) during casting by using of Lost-foam casting (LFC-process) allowed to get samples of zero-dimensional cast composite material (CCM) of the system [Al – FeCr]. Metallographic analysis (MGA) showed that the parameters of the microstructure, such as the specific number of σ-phase inclusions and its dispersion, can vary not only along the height of the cast samples, but are also dependent on each other. Mechanical tests of the obtained material showed that not only the height of the composite casting, but also the parameters of its microstructure affect the temporary resistance to rupture, relative elongation and hardness on the Brinell scale. The application of MGA and mechanical tests for the zero-dimensional CCM of the system [Al – FeCr] and, accordingly, for the control casting showed experimentally what a decrease in the average dispersion of σ-phase inclusions from 26.6 μm to 57.1 μm leads to the fact that the temporary resistance to rupture and the relative elongation of the investigated composite decrease from 135 MPa and 2.5 % to 60 MPa and 0.5 %, respectively. At the same time, the increase in the hardness of samples of the zero-dimensional CCM system [Al – FeCr] from 6.923×10-1 GPa to 7.885×10-1 GPa on the Brinell scale is a consequence of the fact that the average dispersion of σ-phase inclusions in the structure of the studied composite decreases from 26.6 μm to 57.1 μm. The results of the conducted research also made it possible to find out that the increase in the specific number of σ-phase inclusions from 63 mm-2 to 263 mm-2 is the reason for the increase in the temporary resistance to rupture and the relative elongation of the zero-dimensional CCM of the system [Al – FeCr] from 60 MPa and 0.5 % up to 135 MPa and 2.5 %, respectively. However, the hardness of the composite casting, which was determined according to the Brinell scale, and under the condition that the specific number of σ-phase inclusions in the structure of the zero-dimensional CCM of the system [Al – FeCr] is in the range given above, as a result decreases from 7.885×10-1 GPa to 6.923×10-1 GPa.
Bond nature between reinforcing phase and matrix in cast composite material of [Al – FeCr] system and reinforcement mechanism of cast Al-alloys obtained using Lost-foam casting process
The research aims to improve the lost foam casting technology for producing steel bucket teeth for excavators. The relevance of this work lies in the need to enhance the quality of castings in challenging operating conditions, as well as to expand the application of advanced casting technologies within the domestic industry. When analysing the process of manufacturing steel bucket teeth using the lost foam technique, the presence of defects in the castings in the form of shrinkage cavities and gas porosity was detected. Using Flow-3D Cast software, computer simulations of the filling and solidification processes of metal were carried out for two variants of the gating-feeding system, the design of which significantly affects the formation of the quality of castings. The simulation results allowed us to analyse the features of the mold filling with metal for the basic version of the gating-feeding system, identify the risks of gasification products entrapment, and assess the effectiveness of the casting feeding during solidification. Based on the data obtained, an improved design of the gating-feeding system was selected to form a high-quality casting without shrinkage defects. The importance of using polystyrene foam patterns with an optimal density (within 25-30 kg/m³) to minimise the negative consequences of their gasification was also shown. The need to install risers on the patterns that perform the function of “overflows” was substantiated, helping to prevent the formation of defects in the casting. A pilot batch of castings confirmed the effectiveness of the developed technological solutions, which provided the basis for their introduction into the serial production of bucket teeth.
Проведено аналіз вітчизняної та зарубіжної науково-технічної й патентної літератури, а також сформульовано й поставлено мету цієї науково-дослідної роботи (НДР). Шляхом інокулювання ливарного Al-сплаву марки АК12 ДСТУ 2839:1994 дисперсним інтерметалідом FeCr у «порожнині» ливарної форми (ЛФ) при литті за моделями, що газифікуються, одержали зразки нульмірного литого композиційного матеріалу (ЛКМ) системи [Al — FeCr]. За допомогою металографічного аналізу (МГА) вдалося довести, що параметри його мікроструктури (питома кількість включень σ-фази та її дисперсність) не лише змінюються по висоті литих зразків, але й залежать один від одного. Результати випробувань досліджуваного матеріалу на зношування в умовах сухого тертя показали, що триботехнічні властивості {спрацювання матеріалу контртіла (МКТ), зношування ЛКМ системи [Al — FeCr] й коефіцієнт тертя ковзання пари «ЛКМ системи [Al — FeCr] — сталь 40Х»} залежать як від висоти композитного виливка, так і параметрів його мікроструктури. Із застосуванням МГА та внаслідок випробувань в умовах сухого тертя було експериментально доведено, що спрацювання МКТ та коефіцієнт тертя ковзання пари «Al-сплав АК12 — сталь 40Х» внаслідок армування (композиційного зміцнення) ливарного Al-сплаву марки АК12 дисперсним ін- терметалідом FeCr, у середньому, збільшується від 1,15 мг/(см2·км) та 1,77 до 3,75 мг/(см2·км) та 1,98, відповід- но. Натомість його зношування, у середньому, зменшується від 17,85 мг/(см2·км) до 14,15 мг/(см2·км).