The electrical and optoelectronic properties of nanometer-sized ZnO structures are highly influenced by its native point defects. Understanding and controlling these defects are essential for the development of high-performance ZnO-based devices. Here, an electrical device consisting of a polycrystalline ZnO-coated silica nanospring was fabricated and used to characterize the electrical and photoconductive properties of the ZnO layer using near-UV (405 nm) and sub-bandgap (532 and 633 nm) excitation sources. We observe a photocurrent response with all three wavelengths and notably with 532 nm green illumination, which is the energy associated with deep oxygen vacancies. The polycrystalline ZnO-coated silica nanospring exhibits a high responsivity of 1740 A W−1 with the 405 nm excitation source. Physical models are presented to describe the photocurrent rise and decay behavior of each excitation source where we suggest that the rise and decay characteristics are highly dependent on the energy of the excitation source and the trapping of electrons and holes in intermediate defect levels in the bandgap. The energy levels of the trap depths were determined from the photoconductive decay data and are matched to the reported energy levels of singly and doubly ionized oxygen vacancies. A phenomenological model to describe the dependence of the saturation photocurrent on excitation intensity is presented in order to understand the characteristics of the observed breaks in the slopes of the saturation photocurrent versus excitation intensity profile.
We report on the morphological and electrical properties, with (light) and without (dark) UV illumination, of conformal coatings of ZnO on silica nanosprings deposited by sol-gel and atomic layer deposition (ALD) for the first time. Field Emission Scanning Electron Microscopy (FESEM) imaging showed that both methods produce conformal coatings of ZnO on the nanosprings. The surface of the sol-gel coatings exhibited cracks at higher numbers of dipping/sintering cycles, while the morphology of ALD ZnO films were always smooth and devoid of cracks. The effective photoconductivity of the sol-gel ZnO coated nanospring mats increased nonlinearly with increasing coating thickness. The corresponding dark effective conductivity of the sol-gel ZnO coated nanospring mats also increased within the same thickness range. Alternatively, the effective photoconductivity of the ALD ZnO coated nanospring mats increased linearly with increasing coating thickness. The corresponding dark effective conductivity also increased within the same thickness range. The superior effective conductivity and photoconductivity of the ALD ZnO coated nanospring mats is attributed to the uniformity of the coating and the absence of cracks, which are observed for the thicker sol-gel ZnO coatings.