H. Maletta

H. Maletta

Auto-generated profile, based on publicly available information

H. Maletta

Hahn-Meitner-Institut Berlin, Glienicker Straße 100, D-14109 Berlin, Germany

Research Focus & Metrics

Academic Career Length

31Years (1996-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
16 July 2001 in Physical Review B
Verified
Journal Article
Closed access
PDF file
RSR. Sellmann
R. Sellmann
HFH. Fritzsche
H. Fritzsche
HMH. Maletta
H. Maletta
VLV. Leiner
V. Leiner
RSR. Siebrecht
R. Siebrecht
We present a study of the thickness- and temperature-driven spin-reorientation transition in thin epitaxial Au(111)/Co films grown on single-crystal sapphire Al2O3(112¯0) substrates. The transition as a function of Co film thickness was investigated in situ at T=300K by means of the magneto-optical Kerr effect at Co wedge-shaped samples prior and after coverage with W and Au overlayers. The thermal-induced transition, in particular the evolution and stability of in-plane and out-of-plane magnetization components, was studied in the temperature range from 10 to 300 K by reflectivity experiments with polarized neutrons and angular-dependent measurements with superconducting quantum interference device magnetometry. Magnetic phase diagrams, as determined by extended measurements on Au(111)/Co/Au and Au(111)/Co/W show that for the former films the perpendicular anisotropy is stable over a larger thickness region at low temperature.

1 October 1999 in Physical Review B
Verified
Journal Article
Closed access
PDF file
TNT. Nawrath
T. Nawrath
HFH. Fritzsche
H. Fritzsche
FKF. Klose
F. Klose
JNJ. Nowikow
J. Nowikow
HMH. Maletta
H. Maletta
We shall discuss perspectives opened up by using polarized neutron reflectometry as an in situ technique to measure the magnetization of ultrathin films not covered by a protective layer. In order to demonstrate the advantage of this method, Fe(110) films of a thickness of up to 20 Å were prepared on V(110) single crystals. In neutron measurements the absolute value of the magnetization of the films was determined precisely by a simple optical model, by fitting the spin-up and spin-down reflectivities separately. Additionally the measurements were compared with data obtained from magneto-optical Kerr magnetometry. Both techniques show that the magnetizations of the films are considerably reduced.

15 February 2002 in Physical Review B
Verified
Journal Article
Closed access
PDF file
CRCh. Rehm
Ch. Rehm
HMH. Maletta
H. Maletta
MFM. Fieber-Erdmann
M. Fieber-Erdmann
EHE. Holub-Krappe
E. Holub-Krappe
FKF. Klose
F. Klose
Hydrogen absorption in Nb layers of Fe/Nb and W/Nb films was explored in situ by small-angle neutron/ x-ray reflectometry, high-angle x-ray diffraction, and EXAFS spectroscopy. In addition to the hydrogen-induced Nb lattice expansion, the experiments reveal an anomalously large thickness expansion of the Nb layers. This expansion is interpreted to be caused by the rearrangement of Nb atoms, and the creation of additional lattice planes in response to the hydrogen-induced lateral lattice strain. This effect is likely the origin of the extraordinarily large hydrogen concentrations found in these films.

1 November 2002 in Physical Review B
Verified
Journal Article
Closed access
PDF file
JLJ. Langer
J. Langer
JDJ. Hunter Dunn
J. Hunter Dunn
AHA. Hahlin
A. Hahlin
OKO. Karis
O. Karis
RSR. Sellmann
R. Sellmann
HMH. Maletta
H. Maletta
X-ray magnetic circular dichroism vector magnetometry provides evidence that the spin reorientation transition in epitaxially grown Au/Co/Au films depends on the thickness of the Au capping layer. Whereas a 1.9-nm-thick Co film with a 2-nm Au cap exhibits the expected pure in-plane orientation of the magnetization in the remanent state at room temperature, the same film with thinner Au cap shows a significant out-of-plane component. These findings are linked with the observation of a cap-induced enhancement of the orbital moment of about 0.05μB per Co atom.

1 March 1996 in Physical Review B
Verified
Journal Article
Closed access
PDF file
YLYi Li
Yi Li
CPC. Polaczyk
C. Polaczyk
FKF. Klose
F. Klose
JKJ. Kapoor
J. Kapoor
HMH. Maletta
H. Maletta
DRD. Riegel
D. Riegel
Fe films ranging in thickness from 6 to 90 Å have been prepared on Ni layers with constant thickness of 140 Å grown on Si(100) in ultrahigh vacuum. Magnetic properties have been studied by spin-polarized neutron reflection and superconducting quantum interference device magnetometry and structural properties have been investigated by small-angle x-ray reflectometry and reflection high-energy electron diffraction. As the main result of this work it is shown that the magnetic states of the Fe films strongly depend on their thicknesses. For Fe layers ≤32 Å, the average magnetic Fe moments come out to be very low around 0.2μB. For Fe layers ≥60 Å, the Fe moments increase by a factor of about 10 close to the value known for bulk iron. Most probably these changes can be attributed to a structural phase transition of the Fe films from fcc-like to bcc with increasing Fe layer thickness. Fe films below 32 Å are either antiferromagnetic or exhibit almost vanishing Fe moments. The discussion includes a comparison of our results for Fe/Ni bilayers with results published for Fe/Ni multilayers and for Fe films on Cu.

18 May 2001 in Physical Review B
Verified
Journal Article
Closed access
PDF file
GEGeorg Ehlers
Georg Ehlers
HCH. Casalta
H. Casalta
RLR. E. Lechner
R. E. Lechner
HMH. Maletta
H. Maletta
We have studied the dynamics of Tb spins in the intermetallic compound TbNiAl in the paramagnetic (pm) and ordered antiferromagnetic (afm) phases by means of neutron time-of-flight and spin-echo spectroscopy. It is a remarkable and very unusual characteristic of TbNiAl that its afm phase (below TN=47 K) contains regular long-range ordered spins as well as frustrated spins. The latter are identified by a strongly reduced moment measured by neutron diffraction. The new quasielastic measurements show that the frustrated moments relax on a time scale of 0.01 ns to 0.1 ns. Their autocorrelation function I(q,t) is q independent and exponential in time. While in the pm phase the spin relaxation is complete, i.e., I(q,t) goes to zero in the time range of the measurement, in the afm phase I(q,t) stays above zero.