We present a steepest descent energy minimization scheme for micromagnetics. The method searches on a curve that lies on the sphere which keeps the magnitude of the magnetization vector constant. The step size is selected according to a modified Barzilai-Borwein method. Standard linear tetrahedral finite elements are used for space discretization. For the computation of quasistatic hysteresis loops, the steepest descent minimizer is faster than a Landau-Lifshitz micromagnetic solver by more than a factor of two. The speed up on a graphic processor is 4.8 as compared to the fastest single-core central processing unit (CPU) implementation.
The coercive field of permanent magnets decreases with increasing grain size. The grain size dependence of coercivity is explained by a size dependent demagnetizing factor. In Dy free Nd2Fe14B magnets, the size dependent demagnetizing factor ranges from 0.2 for a grain size of 55 nm to 1.22 for a grain size of 8300 nm. The comparison of experimental data with micromagnetic simulations suggests that the grain size dependence of the coercive field in hard magnets is due to the non-uniform magnetostatic field in polyhedral grains.
20 April 2018 in Journal of Physics D: Applied Physics
The coercive field and angular dependence of the coercive field of single-grain permanent magnets are computed using finite element micromagnetics. It is shown that the thickness of surface defects plays a critical role in determining the reversal process. For small defect thicknesses reversal is heavily driven by nucleation, whereas with increasing defect thickness domain wall de-pinning becomes more important. This change results in an observable shift between two well-known behavioral models. A similar trend is observed in experimental measurements of bulk samples, where an Nd-Cu infiltration process has been used to enhance coercivity by modifying the grain boundaries. When account is taken of the imperfect grain alignment of real magnets, the single-grain computed results appears to closely match experimental behaviour.
Finite element micromagnetic simulations are used to compute the temperature-dependent hysteresis properties of Nd2Fe14B permanent magnets in order to assess the influence of a hard (Dy,Nd)2Fe14B shell. The simulations show that the 4 nm thick shell cancels out the reduction in coercivity from an outer defect layer, which is known to exist at the grain boundaries in NdFeB permanent magnets. Activation volumes are computed and shown to depend on the structure's configuration as well as the temperature.