A comparison of the room temperature wear behaviour of untreated low alloy steel surfaces with those containing TiC powders was conducted against an alumina ball. The coefficient of friction, the wear rate and the severity of the damage on the surface were assessed. Incorporation of powders produced a hardness 2.6 times greater and a wear rate 21 times less than the untreated steel. Friction from the third body abrasion and protruding carbides of the processed steel resulted in mild wear with a steady state coefficient friction of 0.4. Both samples showed surface chemical reactivity with the environment as a result of the generation of flash temperature producing an oxide layer, which influenced wear.
7 December 2020 in Journal of Applied Polymer Science
In this work, the effects of adding different filler loadings (520 wt%) of zeolite to the ultra-high molecular weight polyethylene (UHMWPE) matrix on the crystallinity behaviour and tribological properties were studied. The zeolite/UHMWPE composites were fabricated using hot compression moulding. The crystallization behaviour was investigated using differential scanning calorimetry (DSC). The tribological properties were monitored using a Ducom TR-20 pin-on-disc tester under different sliding speeds of 0.209 ms-1 and 0.419 ms-1 and with various applied loads of 5, 10, 15, 20, 25, 30 and 35 N. The worn surfaces of the zeolite/UHMWPE composites were observed under the scanning electron microscope (SEM). The results showed that the addition of zeolite into UHMWPE matrix can effectively enhance the percentage crystallinity of the UHMWPE. 15 wt% zeolite-reinforced UHMWPE composites show the increase of 47% in percentage crystallinity as compared to pure UHMWPE. The wear mass loss of the composites was found to be reduced by the incorporation of zeolite in UHMWPE. In addition, the average coefficient of friction (COF) was also found to decrease with the addition of zeolite. The lowest average COF was obtained by 20 wt% zeolite reinforcements into UHMWPE. Shallower grooves and smoother worn surfaces were observed for zeolite/UHMWPE as compared to pure UHMWPE.
The work aimed to develop surfaces that could resist wear at high temperatures, thus achieving a prolonged component life. Surface modification of a low-alloy steel by incorporating TiC particles has been undertaken by melting the surface using a tungsten inert gas torch. The dry sliding wear behaviour at 600°C of the original and modified surfaces was compared. Microscopic examination of both surfaces showed glazed layers across the wear tracks, with differing amounts of oxide and homogeneity. Extensive wear occurred on the steel surface, which showed deformation of the wear scar tracks and a steadily increased friction coefficient. The TiC addition reduced the wear loss, coinciding with a glazed layer 33% thinner than that on the low-alloy steel sample.