De-Yuan Wei

De-Yuan Wei

Auto-generated profile, based on publicly available information

De-Yuan Wei

Hebei Key Lab of Optic-Electronic Information and Materials, Hebei University, Baoding 071002, China

Research Focus & Metrics

Academic Career Length

15Years (2012-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 July 2012 in Journal of Applied Physics
Verified
Journal Article
Open access
PDF file
HZH. P. Zhou
H. P. Zhou
DWD. Y. Wei
D. Y. Wei
SXShengzhi Xu
Shengzhi Xu
SXShaoqing Xiao
Shaoqing Xiao
LXL. X. Xu
L. X. Xu
MXM. Xu
M. Xu
Amorphous and microcrystal hydrogenated intrinsic silicon (a-Si:H/μc-Si:H) thin films with good silicon surface passivation effect were deposited using a precursor gases of silane and hydrogen, which were discharged by low frequency inductively coupled high density plasma source. With regard to silicon surface passivation, the effect of discharge power on thin films properties, including the optical band gap, the crystal fraction, and bond configuration, as well as the deposition rate were thoroughly investigated. It was found that the best passivation effect was obtained at the region near the transition regime from a-Si:H to μc-Si:H with a minimized incubation layer between the passivation layer and substrate. Cz-silicon wafer passivated by as-deposited μc-Si:H thin films without any post-deposition thermal annealing possesses minority carrier lifetime of about 234 μs. This is attributed to the chemical annealing from the high-density hydrogen plasma during the deposition process. Subsequent thermal annealing in hydrogen flow increased the lifetime to 524 μs with a suppressed maximum surface recombination velocity of as low as 60 cm/s. Throughout the process flow covering the pre-deposition H plasma treatment, the film deposition from H2 diluted feedstock gases and the post-deposition annealing, hydrogen plays a vital role to enhance the minority carrier lifetime by improving the interface properties. The injection level dependent surface recombination velocity was also extracted from the lifetime measurement. The effectivity of the a-Si:H/μc-Si:H for silicon surface passivation in a practical heterojunction solar cell was further validated by the excellent photovoltaic performance.

1 January 2012 in Thin Solid Films
Verified
Journal Article
Closed access
WYW.S. Yan
W.S. Yan
DWD.Y. Wei
D.Y. Wei
YGY.N. Guo
Y.N. Guo
SXS. Xu
S. Xu
TOT.M. Ong
T.M. Ong
CSC.C. Sern
C.C. Sern

1 January 2019 in Acta Physica Sinica
Verified
Journal Article
Closed access
PDF file
RHRen He
Ren He
YLYing-Ye Li
Ying-Ye Li
JCJing-Xin Chen
Jing-Xin Chen
XZXue-Ling Zhao
Xue-Ling Zhao
HTHuan Tang
Huan Tang
LCLtd. Yingli Green Energy Holding Co.
Ltd. Yingli Green Energy Holding Co.
用三点弯曲和四点弯曲测试方法分别测试了单晶硅片和双面电池两种不同样片的机械性能, 通过建立模型, 探讨了不同的弯曲测试方法对样片的最大弯曲位移、最大载荷和断裂强度的影响. 研究表明: 三点弯曲和四点弯曲测试测量的最大弯曲位移相差不大, 但对单晶硅片而言, 三点弯曲测试方法测量结果离散度较大, 四点弯曲测试方法测量结果离散度较小. 然而不论是单晶硅片还是双面电池, 四点弯曲测试方法均能通过分散载荷的方式而增加样片的承载能力, 四点弯曲测试方法计算得出的断裂强度较小于三点弯曲测试的结果.

25 June 2019 in IEEE Journal of Photovoltaics
Verified
Journal Article
Closed access
ZHZhiping Huang
Zhiping Huang
WHWentao Hu
Wentao Hu
DZDong Zhang
Dong Zhang
XLXiaowei Li
Xiaowei Li
JCJingwei Chen
Jingwei Chen
YXYing Xu
Ying Xu

14 August 2019 in IEEE Journal of Photovoltaics
Verified
Journal Article
Closed access
RHRen He
Ren He
JCJingwei Chen
Jingwei Chen
DWDeyuan Wei
Deyuan Wei
ZHZhiping Huang
Zhiping Huang
DSDengyuan Song
Dengyuan Song
YXYing Xu
Ying Xu
Cost reduction and efficiency promotion are well-known development directions faced by the photovoltaic industry, and the thin Si solar cell has been identified as a potential candidate to conquer the field. In this article, 120-μm-thick p-type thin multicrystalline silicon (mc-Si) solar cells with a structure based on a full Al back surface field and an efficiency comparable to 180-μm-thick solar cells were fabricated using a conventional production line. The mechanical strength and light-induced degradation effect for the 120-μm-thick mc-Si solar cells were investigated. Our study shows that 120-μm-thick mc-Si cells have greater mechanical strength with a bending displacement of 15.87 mm compared with 180-μm-thick solar cells (7.87 mm), which can facilitate the development of advanced flexible solar cell modules. An important finding of this work is that thin mc-Si solar cells show a weaker light-induced degradation (LID) effect than 180-μm-thick solar cells. A ∼ 2.7% (relative) degradation in efficiency (η) was observed for the 120-μm-thick thin mc-Si solar cells following a one month exposure test. A thin Si solar cell with a promising new type of structure may also be expected to achieve a high η, a low LID effect, and a flexible capability in the near future.