Department of Physics, Chair for Functional Materials, TUM School of Natural Sciences, Technical University of Munich, James-Franck-Str. 1, Garching 85748 Germany
Auto-generated profile, based on publicly available information
Linus F. Huber
Department of Physics, Chair for Functional Materials, TUM School of Natural Sciences, Technical University of Munich, James-Franck-Str. 1, Garching 85748 Germany
Reduced‐dimensional perovskites (RDPs) have advanced perovskite optoelectronic devices due to their tunable energy landscape, structure, and orientation. However, the origin of structural and photophysical property changes when moving from low‐dimensional to high‐dimensional RDPs remains to be understood. This study systematically reveals structural and photophysical properties of slot‐die‐coated Dion‐Jacobson (DJ) and Ruddlesden‐Popper (RP) RDPs with different dimensionalities. RP RDPs with lower dimensionality (n = 2) exhibit a dominant n = 2 phase, preferential out‐of‐plane orientation, and longer charge carrier lifetime compared with DJ RDPs. In addition, the formation kinetics of RDPs with higher dimensionality (n = 4) are unraveled by in situ X‐ray scattering, showing the favorable formation of the lower‐n phase in RP RDPs. The formation of these lower‐n phases is thermodynamically and stoichiometrically favored, while these phases are likely in the form of an “intermediate phase” which bridges the 3D‐like and lower‐n phases in DJ RDPs. DJ RDPs with higher dimensionality demonstrate comparable phase purity, preferential orientation, spatially vertical phase homogeneity, and longer charge carrier lifetime. As such, DJ‐based perovskite solar cells (PSCs) (n = 4) demonstrate better photostability under operational conditions than RP‐based PSCs. Thus, the work paves the way for the utilization of RDPs to upscale PSCs.
The whey protein beta-lactoglobulin (β-lg) is used as a biotemplate for the water-based synthesis of nanostructured and foam-like titania films based on its variation in supramolecular structure when denatured at different pH values. Acting as a matrix, β-lg is mixed with the water-soluble titania precursor Ti(IV) bis(ammonium lactate)dihydroxide (TiBALDh) to promote biotemplated titania precipitation. Since TiBALDh is in chemical equilibrium with anatase titania nanoparticles and Ti(IV)-lactate complexes, and this equilibrium shifts with varying pH, the influence of the pH value on the final film morphology becomes essential. This work investigates this influence for three pH values: pH 7, pH 5, i.e., close to the isoelectric point of β-lg, and pH 2. Spray coating, a method of industrial relevance, is used to fabricate biohybrid β-lg:TiBALDh foam-like films. The obtained films are calcined to combust biotemplate β-lg and achieve nanostructured titania films. To understand the influence of pH on the film morphology, grazing-incidence small-angle and wide-angle X-ray scattering (GISAXS/GIWAXS) and grazing-incidence small-angle neutron scattering (GISANS), in combination with scanning electron microscopy (SEM), are applied to both the biohybrid and biotemplated titania films. With these techniques, information about domain sizes, porosity, and crystal structure is obtained with high statistical significance. Fourier-transform infrared spectroscopy (FTIR) probes the interaction of TiBALDh and β-lg on the molecular level as a function of pH. The results underline pH as a suitable tool for tuning the morphology in biotemplated titania films.
The thermoelectric properties of fully sprayed thin films of poly(3-hexylthiophen-2,5-diyl) (P3HT) doped with chloroauric acid are investigated for different film thicknesses. The film thickness increases logarithmically with increasing amount of deposited material on the surfaces. Both the electrical conductivity and measured Seebeck coefficients of the doped thin films show an optimal polymer layer thickness between 275 and 310 nm and yield a maximum power factor of $$(1.77\,\pm \,0.22) \frac{\mu \text {W}}{\text {m}\cdot \text {K}^2}$$ . The optimum layer thickness results from the optimal amount of dopant molecules per monomer between 1.1 and 1.3 at these ratios of P3HT and HAuCl $$_4$$ for the thin film fabrication.