Jing Li

Jing Li

Auto-generated profile, based on publicly available information

Jing Li

Department of Physics and Atmospheric Science, Dalhousie University, Halifax, Nova Scotia B3H 3J5, Canada

Research Focus & Metrics

Academic Career Length

14Years (2013-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
17 April 2015 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
JLJing Li
Jing Li
LDLaura E. Downie
Laura E. Downie
LMLin Ma
Lin Ma
WQWenda Qiu
Wenda Qiu
JDJ. R. Dahn
J. R. Dahn
LiNi0.8Mn0.1Co0.1O2 (NMC811) can deliver a high capacity of ∼200 mAh/g with an average discharge potential of ∼3.8 V (vs. Li+/Li), making it a promising positive electrode material for high energy density lithium ion batteries. However, electrochemical tests from half cells and full cells show poor cycling performance when charged to potentials above 4.2 V. The calendar and cycle lifetimes of cells are affected by the structural stability of the active electrode materials as well as the parasitic reactions that occur in lithium ion batteries. In order to explore the major failure mechanisms of the material, half cells (coin cells) with control electrolyte and full cells (pouch cells) with control electrolyte and with selected electrolyte additives were tested over four different potential ranges. Isothermal microcalorimetry was used to explore the parasitic reactions and their potential dependence. In-situ and ex-situ X-ray diffraction and scanning electron microscopy were used to investigate the structural and morphological degradation of the materials over cycling. It was found that the dramatic c-axis change of the active material during charge and discharge may not be the major problem for cells that are cycled to higher potentials. The parasitic reactions that arise from the interactions between the electrolyte and the highly reactive delithiated cathode surface at high potentials are suggested as the main reason for the failure of cells cycled above 4.2 V. It should be possible to further improve the performance of NMC811 at high potentials by modifying the cathode surface and/or identifying and using electrolyte blends which reduce parasitic reactions.

20 September 2018 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
HLHongyang Li
Hongyang Li
NZNing Zhang
Ning Zhang
JLJing Li
Jing Li
JDJ. R. Dahn
J. R. Dahn
Ni-rich transition metal layered oxide materials are of great interest as positive electrode materials for lithium ion batteries. As the popular electrode materials NMC (LiNi1-x-yMnxCoyO2) and NCA (LiNi1-x-yCoxAlyO2) become more and more Ni-rich, they approach LiNiO2. Therefore it is important to benchmark the structure and electrochemistry of state of the art LixNiO2 for the convenience of researchers in the field. In this work, LiNiO2 synthesized from a commercial Ni(OH)2 precursor and modern synthesis methods shows a specific capacity close to the theoretical specific capacity of 274 mAh/g. In-situ X-ray diffraction (XRD) measurements were conducted to obtain accurate structural information versus lithium content, x. The known multiple phase transitions of LixNiO2 during charge and discharge were clearly observed, and the variation in unit cell lattice constants and volume was measured. Differential capacity versus voltage (dQ/dV vs. V) studies were used to investigate the electrochemical properties including regions of composition that show very slow kinetics. It is hoped that this work will be a useful reference for those working on Ni-rich positive electrode materials for Li-ion cells.

15 March 2018 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
HLHongyang Li
Hongyang Li
JLJing Li
Jing Li
XMXiaowei Ma
Xiaowei Ma
JDJ. R. Dahn
J. R. Dahn
Single crystal LiNi0.5Mn0.3Co0.2O2 (NMC532) was shown to have superior stability at high voltages and elevated temperatures compared to conventional polycrystalline NMC532 by the authors. Conventional LiNi0.6Mn0.2Co0.2O2 (NMC622) usually offers more capacity than NMC532 when charged to the same upper cutoff voltage so NMC622 is attractive. It is expected that single crystal NMC622 could also provide better performance than typical polycrystalline NMC622 materials. This work explores the synthesis of single crystal LiNi0.6Mn0.2Co0.2O2 and preferred synthesis conditions were found. A washing and reheating method was used to remove residual lithium carbonate after sintering. The synthesized single crystal NMC622 material worked poorly after the washing-heating treatment without the use of electrolyte additives in the electrolyte. However, with selected additives, single crystal cells outperformed the polycrystalline reference cells in cycling tests. It is our opinion that single crystal NMC622 has a bright future in the Li-ion battery field.

15 November 2017 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
JLJing Li
Jing Li
HLHongyang Li
Hongyang Li
WSWill Stone
Will Stone
RWRochelle Weber
Rochelle Weber
SHSunny Hy
Sunny Hy
JDJ. R. Dahn
J. R. Dahn
Single crystal Li[Ni0.5Mn0.3Co0.2]O2 materials in NMC532/artificial graphite cells have excellent long term charge-discharge cycle lifetime which greatly exceeds that of conventional NMC532 materials. There are a few patents from industry regarding the synthesis of single crystal NMC. In addition, there have only been a few reports in the academic literature showing that single crystal NMC with a grain size of ∼2–5 μm having good electrochemical performance was successfully synthesized, but these workers used complex approaches. This work systematically studies the steps required to synthesize single crystal NMC materials. The key synthesis steps including the impact of the Li to transition metal ratio, sintering temperature, precursor size and sintering time are discussed. This work provides guidance for the synthesis of single crystal NMC positive electrode materials that may be suitable for lithium-ion cells with high energy density and long lifetime.

21 December 2015 in Chemistry of Materials
Verified
Journal Article
Closed access
JLJing Li
Jing Li
RSRamesh Shunmugasundaram
Ramesh Shunmugasundaram
RDRenny Doig
Renny Doig
JDJ. R. Dahn
J. R. Dahn

23 August 2018 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
JLJing Li
Jing Li
JHJessie Harlow
Jessie Harlow
NSNikolai Stakheiko
Nikolai Stakheiko
NZNing Zhang
Ning Zhang
JPJens Paulsen
Jens Paulsen
JDJ. R. Dahn
J. R. Dahn
The dependence of differential capacity versus voltage (dQ/dV) of Li/NCA half cells on temperature and testing current (C-rate) was studied. Kinetic hindrance of lithium diffusion at both low (∼3.5 V vs Li/Li+) and high states of charge (∼4.17 V) was observed. In-situ X-ray diffraction measured the volume changes of the NCA lattice versus state of charge. NCA/graphite pouch cells were cycled in various voltage ranges to explore the impacts of depth of discharge (DOD) ranges and the kinetic hindrance regions in NCA on cell failure. dV/dQ analysis, full cell impedance and symmetric cell impedance analysis as well as half-cell studies of recovered electrodes were performed after 0, ∼400 and 800 charge-discharge cycles. The contributions of active mass loss and shift loss (from loss of Li inventory) to the capacity fade of NCA/graphite cells under various testing conditions were determined. The increase in positive electrode charge transfer impedance with cycle number was proportional to the increase of positive electrode active mass loss. There was no strong correlation between positive electrode active mass loss and lattice volume change. NCA active mass loss during cycling can be minimized when the dQ/dV peaks at ∼3.5 and 4.17 V (vs. Li/Li+), that show kinetic hindrance, are partially or completely avoided.