16 November 2017 in Scientific Reports
Phenomena occurring in duplex lightweight steels under dynamic loading are hardly investigated, although its understanding is essentially needed in applications of automotive steels. In this study, quasi-static and dynamic tensile properties of duplex lightweight steels were investigated by focusing on how TRIP and TWIP mechanisms were varied under the quasi-static and dynamic loading conditions. As the annealing temperature increased, the grain size and volume fraction of austenite increased, thereby gradually decreasing austenite stability. The strain-hardening rate curves displayed a multiple-stage strain-hardening behavior, which was closely related with deformation mechanisms. Under the dynamic loading, the temperature rise due to adiabatic heating raised the austenite stability, which resulted in the reduction in the TRIP amount. Though the 950 °C-annealed specimen having the lowest austenite stability showed the very low ductility and strength under the quasi-static loading, it exhibited the tensile elongation up to 54% as well as high strain-hardening rate and tensile strength (1038 MPa) due to appropriate austenite stability under dynamic loading. Since dynamic properties of the present duplex lightweight steels show the excellent strength-ductility combination as well as continuously high strain hardening, they can be sufficiently applied to automotive steel sheets demanded for stronger vehicle bodies and safety enhancement.
1 February 2019 in Fuel Processing Technology
1 March 2022 in International Journal of Fatigue
1 February 2016 in Metallurgical and Materials Transactions A
In this study, dynamic tensile properties of dendrite-containing Ti-based amorphous matrix composites were examined, and effects of dendrite size on dynamic deformation were investigated. The composites contained 73 to 76 vol pct of dendrites whose effective sizes were varied from 63 to 103 μm. The dynamic tensile test results indicated that the ultimate tensile strength increased up to 1.25 GPa, whereas the elongation decreased to 1 pct, although the overall strength and elongation trends followed those of the quasi-static tensile test. According to the observation of dynamic tensile deformation behavior, very few deformation bands were observed beneath the fracture surface in the composite containing large dendrites. In the composite containing small dendrites, deformation bands initiated inside small dendrites propagated into adjacent dendrites through the amorphous matrix, and were crossly intersect perpendicularly in widely deformed areas, which beneficially worked for elongation as well as strength.