Novel environment-friendly NaNbO 3 -based lead-free ceramics with ultrahigh energy storage density and power density for multilayer ceramic capacitor applications.
19 September 2018 in Journal of Materials Chemistry C
Bismuth ferrite (BiFeO3, BFO) possesses very large spontaneous polarization, which provides a great potential in dielectric energy-storage capacitors. However, the presence of large remanent polarization heavily restricts the achievement of excellent performance in the energy storage field. Herein we designed local compositional disorder and constructed quenched random fields to maximize the discrepancy between the maximum polarization and the remanent polarization by means of introducing Zn2+ and Ta5+ at B-sites together in BiFeO3-based solution. Interestingly, pinched-hysteresis loops were observed in this Ba(Zn1/2Ta2/3)O3-modified BFO-based solution. Ultrahigh recoverable energy density (2.56 J cm−3) was first reported under low electric field (16 kV mm−1), which is much superior to the previous results regarding BFO-based bulk ceramics. In addition, an excellent recoverable energy density (>2 J cm−3) and a high efficiency (>80%) were obtained simultaneously in this BZT-modified BFO-based bulk material under low electric field (<20 kV mm−1). These results demonstrate that the strategy of constructing weakly coupled polar structures is feasible and effective to boost the energy density and efficiency for BiFeO3-based bulk ceramics, which may pave a significant step towards utilizing energy-storage applications for BiFeO3-based materials.
Recently, dielectric capacitors have drawn much attention from researchers and engineers due to their ultrahigh power density, ultrafast charge–discharge rate, and good temperature and fatigue stability. However, most related research mainly focuses on the improvement in dielectric breakdown strength and energy storage density rather than that in energy efficiency. In this study, we adopted the spark plasma sintering method to modify the microstructure and electric conductivity of Na0.7Bi0.1NbO3 lead-free ceramics, and subsequently enhanced their energy storage properties. As a result, the Na0.7Bi0.1NbO3 ceramics prepared by the spark plasma sintering method display a considerably large energy storage density of 3.41 J cm−3 with an ultrahigh energy storage efficiency of 90.8% at 28 kV mm−1. The improvement of energy storage performance is ascribed to the reduction of electric conductivity, which can be analyzed by the X-ray photoelectron spectroscopy and high-temperature complex impedance spectra. This study not only paves the way for environment-friendly Na0.7Bi0.1NbO3 lead-free ceramics to be developed for energy storage applications, but also interprets the internal mechanism of microstructure modulation which enhances energy storage properties.
16 March 2022 in ACS Applied Materials & Interfaces