1 March 2021 in Journal of the Mechanical Behavior of Biomedical Materials
Verified
Journal Article
Closed access
AGAnastasiia Grymak
Anastasiia Grymak
JAJohn M. Aarts
John M. Aarts
SMSunyoung Ma
Sunyoung Ma
JWJohn Neil Waddell
John Neil Waddell
JCJoanne Choi
Joanne Choi

13 September 2021 in Journal of Prosthodontics
Verified
Journal Article
Closed access
PDF file
AGAnastasiia Grymak
Anastasiia Grymak
JAJohn M. Aarts
John M. Aarts
SMSunyoung Ma
Sunyoung Ma
JWJ. Neil Waddell
J. Neil Waddell
JCJoanne Choi
Joanne Choi

12 June 2024 in Journal of Dentistry
Verified
Journal Article
Open access
AGAnastasiia Grymak
Anastasiia Grymak
JAJohn M Aarts
John M Aarts
ACAndrew B Cameron
Andrew B Cameron
JCJoanne Choi
Joanne Choi
To evaluate the wear resistance of three additively manufactured dental crown materials (NextDent C&B MFH, Saremco print CROWNTEC and Bego VarseoSmile Crown) under two environmental conditions (dry and artificial saliva), two loads (49 N and 70 N) and two surface treatments (polished and glazed). A total of 120 specimens were divided into 24 groups and tested for wear under two loads (49 N and 70 N), surface treatment (polished or glazed), and environment (dry or submerged in artificial saliva). All samples underwent reciprocating wear testing at 1 Hz using a wear simulator, replicating 48 months of In Vivo conditions with a stainless-steel ball as the antagonist. The coefficient of friction (CoF), surface roughness, volumetric and vertical wear loss were measured and statistically analysed. Confocal microscopy assessed the surface properties of crown materials and the antagonists. The NextDent material demonstrated the most homogenous wear, with relatively low vertical and volumetric loss across all groups (p < 0.004). NextDent and Bego materials performed similarly in artificial saliva regardless of the load type (p > 1.000). The CoF remained below 0.3 for all groups. All groups exhibited significant increases in surface roughness after testing, however, this did not correlate with an increase in the CoF. Confocal analysis revealed material deformities due to load and notable scratch marks on the stainless-steel antagonists. It was found that all investigated addtively manufactured materials can be suggested for provisional use. Both vertical loss and volumetric loss results should be included for material evaluation. CoF and surface roughness should be implemented into wear evaluation. This study highlights the practical value of additively manufactured dental crown materials, particularly for provisional restorations. However, their extended use requires careful consideration of individual patient needs, emphasising the need for judicious clinical application evaluation.

1 December 2021 in Journal of the Mechanical Behavior of Biomedical Materials
Verified
Journal Article
Closed access
GLGray Hun Li
Gray Hun Li
SCShiyao Chen
Shiyao Chen
AGAnastasiia Grymak
Anastasiia Grymak
JWJohn Neil Waddell
John Neil Waddell
JKJohn Jungki Kim
John Jungki Kim
JCJoanne Choi
Joanne Choi

18 February 2022 in Oral
Verified
Journal Article
Open access
PDF file
MPMei Ting Pong
Mei Ting Pong
AGAnastasiia Grymak
Anastasiia Grymak
JWJohn Neil Waddell
John Neil Waddell
JCJoanne Choi
Joanne Choi
Aim: To measure the bond strength between two different CAD/CAM PMMA denture base resins and three different types of gum characterisation composites. Materials and Methods: CAD/CAM single cross-linked (Telio CAD) and double cross-linked (Vivodent CAD) resins were prepared, obtaining a total of 180 bar specimens. Each specimen was prepared according to the manufacturer’s instructions. The specimens were bonded to three different characterisation composites with varying viscosities; Kulzer Pala-creactive (P), Ivoclar SR Nexco (S), Shofu Ceramage (F). All the specimens were then tested using a chevron-notched three-point bond strength test in a universal testing machine to obtain fracture energy release toughness (MPa√m) and bond strength (MPa). The specimens were thermocycled to simulate 6 and 12 months of ageing in vivo. The results were statistically analysed (SPSS). The fractured surfaces of the tested specimens were examined with a scanning electron microscope (SEM) to evaluate the failure modes. Results: Pala-creactive characterisation composites showed the highest overall bond strength (3.49 ± 0.86 MPa) and fracture toughness (1.59 ± 0.34 MPa√m) when bonded to both CAD PMMA denture resins, which were statistically higher than the values obtained when they were bonded to Telio (p < 0.001). The Ceramage composite showed the lowest bond strength (1.05 ± 0.59 MPa) and fracture toughness (0.47 ± 0.4 MPa√m). The dominant mode of failure for all groups was mixed. Conclusion: Single cross-linked PMMA (Telio) showed a higher overall bond strength compared to double cross-linked PMMA when bonded to three different characterisation composites. Telio CAD showed a clear bond strength decrease after 6 and 12 months of artificial ageing, while Vivodent CAD showed a bond strength increase.

15 June 2022
Verified
Journal Article
Open access
PDF file
TSTsz Ho Seto
Tsz Ho Seto
AGAnastasiia Grymak
Anastasiia Grymak
VMVidya Latchmi Mudliar
Vidya Latchmi Mudliar
JCJoanne Choi
Joanne Choi
The increase in aesthetic demands has increased the use of ceramic dental restorations in dentistry. Ceramic restorations are bonded to the tooth structure using adhesives. There is a lack of standard guidelines in terms of post-bleaching time intervals and bond strengths of ceramic restorations. Bleaching products have also been stated to affect the morphology of enamel. Therefore, the purpose of this systematic review is to evaluate the bond strength between ceramic and enamel and the changes in the surface roughness of enamel post teeth bleaching. An electronic search was performed in the databases PubMed, OVID MEDLINE, Scopus, and Web of Science with MESH terms: “adhesion OR bonding”, “ceramic OR ceramics OR dental porcelain”, “tooth bleaching OR teeth bleaching OR tooth whitening OR teeth whitening” and “enamel OR dental enamel OR enamels OR dental enamels”. The articles were screened, and the final selection of articles was obtained by using the inclusion and exclusion criteria. Of the 170 studies identified from the search, only 12 studies met the inclusion criteria and were selected for full-text review. A further search by hand was performed, and additional 48 studies were selected. From the 60 full-text studies, 18 studies met the inclusion criteria and were included for data extraction. The results were based on a descriptive analysis of the effect on bond strength of ceramic to enamel after a bleaching protocol and the changes in the surface roughness of enamel post bleaching protocol. In conclusion, bleaching protocols alter the surface roughness of enamel and, thus, the shear bond strength between ceramic and enamel. Bleaching treatments with a higher concentration of hydrogen peroxide reduce the bond strength between ceramic and enamel. Delaying bonding after bleaching for up to 7 days increases the bond strength between ceramic and enamel.