1 July 2011 in Thin Solid Films
17 March 2014 in Applied Physics Letters
The orientation dependence of the piezoresistive effect of p-type single crystalline 3C-SiC thin film grown on a (100)Si wafer was characterized. The longitudinal, transverse gauge factors in [100] orientation, and longitudinal gauge factor in [110] orientation were found to be 5.8, −5.2, and 30.3, respectively. The fundamental piezoresistive coefficients π11, π12, and π44 of p-type 3C-SiC were obtained to be 1.5 × 10−11 Pa−1, −1.4 × 10−11 Pa−1, and 18.1 × 10−11 Pa−1, respectively. From these coefficients, the piezoresistive effect in any crystallographic orientation in p-type single crystalline 3C-SiC can be estimated, which is very valuable in designing micro-mechanical sensors.
7 January 2013 in Applied Physics Letters
Residual stresses in epitaxial 3C-SiC films on silicon, for chosen growth conditions, appear determined by their growth orientation. Stress evaluation locally with Raman spectroscopy, and across a 150 mm wafer with curvature measurements, indicate that thin films can be grown on Si(100) with residual tensile stresses as low as 150 MPa. However, films on Si(111) retain a considerably higher stress, around 900 MPa, with only minor decrease versus film thickness. Stacking faults are indeed geometrically a less efficient relief mechanism for the biaxial strain of SiC films grown on Si(111) with 〈111〉 orientation. Residual stresses can be tuned by the epitaxial process temperatures.
1 August 2011 in Journal of Crystal Growth
18 July 2014 in Journal of Materials Chemistry C
The influence of crystal defects on the gauge factor of p-type single crystalline 3C-SiC thin films is reported.
31 January 2014 in IEEE Electron Device Letters
This letter presents for the first time the piezoresistive effect of p-type single crystalline 3C-SiC thin film. The 3C-SiC thin film was epitaxially grown on (100) p-type Si substrate using the low-pressure chemical vapor deposition process. The grown 3C-SiC was doped in situ with aluminum to form p-type semiconductor with carrier concentration of 5×10 18 cm -3 and sheet resistance of about 40 kΩ/□. Longitudinal and transverse gauge factors (GFs) of the 3C-SiC in [110] orientation at room temperature (23°C) were 30.3 and -25.1, respectively. These results indicated that the p-type single crystalline 3C-SiC possessed a higher GF than the previously reported results in p-type polycrystalline 3C-SiC.