1 July 2019 in Journal of Alloys and Compounds
3 July 2020 in IEEE Photonics Technology Letters
AlGaN-based 300-nm ultraviolet (UV) light-emitting diodes (LEDs) with various p-n junction mesa perimeter-to-area (P/A) ratios and mesa depths were fabricated. As the mesa P/A ratio increases from $0.0133\,\,\mu \text{m}^{-1}$ to 0.157 $\mu \text{m}^{-1}$ and the mesa depth increases from 550 nm to 1700 nm, the peak external quantum efficiency (EQE) increases from 2.93% to 4.89%. Fitting results from the ABC+f(n) model reveal that the light-extraction efficiency (LEE) is the major factor limiting the EQE, which can be enhanced by increasing the mesa P/A ratio and mesa depth. On the other hand, increasing the mesa P/A ratio and mesa depth also leads to increased Auger recombination coefficient from $1.11\times 10^{-31}$ cm $^{6}\text{s}^{-1}$ to $2.11\times 10^{-30}$ cm $^{6}\text{s}^{-1}$ , and the probable mechanism is defect-assisted Auger recombination at mesa sidewall by etching damage. In spite of the decreased internal quantum efficiency by Auger recombination, the improved LEE by increasing the mesa P/A ratio and mesa depth is still the major factor for the EQE at the current density below 150 A/cm 2 for UV LEDs.
1 March 2019 in Journal of Alloys and Compounds