In this article, the copper-chromium-zirconium (CuCrZr) alloys plates with 21 mm in thickness were butt joined together by means of FSW (friction stir welding). The properties of the FSW joints are studied. The microstructure variations during the process of FSW were investigated by optical microscopy (OM), electron back-scattered diffraction (EBSD), and transmission electron microscopy (TEM). The results show that the grains size in the nugget zone (NZ) are significantly refined, which can be attributed to the dynamic recrystallization (DRX). The microstructure distribution in the NZ is inhomogeneous and the size of equiaxed grains are decreased gradually along the thickness direction from the top to bottom area of the welds. Meanwhile, it is found that the micro-hardness and tensile strength of the welds are slightly increased along the thickness direction from the top to the bottom area of the welds. All the nano-strengthening precipitates in the BM are dissolved into the Cu matrix in the NZ. Therefore, the decreases in hardness, tensile strength, and electrical conductivity can be attributed to the comprehensive effect of dissolution of nano-strengthening precipitates into the supersaturation matrix and severe DRX in the welded NZ.
In this study, dissimilar CuNiCrSi and CuCrZr butt joints were friction stir welded at a constant welding speed of 150 mm/min, but at different rotational speeds of 800, 1100, 1400, 1700, and 2100 rpm. Sound joints were achieved at the rotational speeds of 1400 and 1700 rpm. It was found that the area of retreating material and grain size in the nugget zone increased with the increase of tool rotational speeds. The base metal on the CuNiCrSi side (CuNiCrSi-BM) contains a large density of Cr and δ-Ni2Si precipitates, and a great deal of Cr precipitates can be observed in the base metal on the CuCrZr side (CuCrZr-BM). All these precipitates are completely dissolved into the matrix in both the nugget zone on the CuCrZr side (CuCrZr-NZ) and the nugget zone on the CuNiCrSi side (CuNiCrSi-NZ). The precipitation strengthening plays a dominant role in the base metals, but the grain boundary strengthening is more effective in improving the mechanical properties in the nugget zone. Both the hardness and tensile strength decrease sharply from the base metal to the nugget zone due to the dissolution of precipitates. Mechanical properties such as microhardness and tensile strength in the nugget zone decrease with the increase of rotational speeds because the grain size is larger at a higher rotational speed.
Despite its significance in practical applications, until today dissolutive wetting in metallic systems remains poorly understood due to the intricate liquid/solid interactions. In this study, we investigate nine metallic systems encompassing a vast range of thermodynamic behaviors. Our findings reveal three distinct wetting behaviors and identify two key thermodynamic parameters that control solid solution formation and then dissolutive wetting behaviors, namely the solubility of the substrate element in the liquid ( $${C}_{L}$$ ) and the solidification composition range ( $${C}_{R}$$ ). We observe a slow spreading due to the step flow mechanism in systems with a relatively low $${C}_{L}$$ and narrow $${C}_{R}$$ . For systems with high $${C}_{L}$$ , the spreading begins relatively fast and transitions to the step flow mechanism when $${C}_{L}$$ is reached. Systems with a large $${C}_{R}$$ , conversely, exhibit consistently fast spreading. Density functional theory (DFT) calculations provide deeper insights into the underlying atomistic mechanisms affecting the solid solution formation. Our results offer inspiration for optimizing high-temperature processing techniques, such as welding, coating and high temperature infiltrating.
30 October 2024 in Case Studies in Thermal Engineering