The SEI films formation/composition were dominated by VC resulting in better electrochemical performance of LiNi 1/3 Mn 1/3 Co 1/3 O 2 (NMC)/graphite pouch cells.
2 October 2015 in Journal of the Electrochemical Society
The role of prop-1-ene-1,3-sultone (PES) used alone or in combination with vinylene carbonate (VC) in LiNi1/3Mn1/3Co1/3O2(NMC)/graphite pouch cells was studied by correlating data from differential capacity (dQ/dV) analysis, gas chromatography/mass spectroscopy (GC−MS), ultrahigh precision coulometry, storage experiments and X-ray photoelectron spectroscopy. VC formed more stable and protective SEI films at both graphite and NMC surfaces due to the formation of a polymer of VC. For PES-containing electrolytes, the preferential reaction of PES led to the formation of SEI films with higher oxygen content at both graphite and NMC surfaces due to the additional oxygen contribution of sulfite species and substantially less LiF compared to control and VC electrolytes. PES also led to thicker SEI films at the NMC surface. When VC was combined with PES, features of the SEI films from both VC and PES were observed. The SEI film features for VC and PES used alone or in combination can explain the improved electrochemical performance as well as the lower production of gas observed with these additives compared to control electrolyte.
23 November 2021 in ACS Applied Materials & Interfaces
The effects of a ternary electrolyte additive system on Li[Ni0.42Mn0.42Co0.16]O2 (NMC442)/graphite pouch cells balanced for 4.7 V was thoroughly investigated. The additive system consisted of 2% prop-1-ene-1,3-sultone (PES) + 1% methylene methane disulfonate + 1% tris-(trimethylsilyl)-phosphite (TTSPi) which is denoted “PES211”. “PES211” significantly improved the capacity retention, impedance and gas evolution of NMC442/graphite pouch cells cycled at constant current up to 4.4 V or 4.5 V. X-ray photoelectron spectroscopy results suggest more stable and passivating SEI films at both graphite and NMC442 surfaces due to the preferential electrochemical reaction of PES and MMDS as well as the preferential chemical reaction of TTSPi at the graphite surface. “PES211” modifies the reactivity of the LiPF6 salt at the graphite surface and hinders its degradation at high potential. However, during extended exposure to 4.5 V, less passivating SEI films were observed leading to extensive electrolyte degradation, capacity loss, impedance increase and gas evolution even for NMC442/graphite pouch cells containing “PES211”.